Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Mold Temperature = 20.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Multibase TPSiV® 4000-50A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
Mold Temperature 20.0 - 60.0 °C
68.0 - 140 °F
Polykemi AB POLYelast TPE EC88R Thermoplastic Elastomer, PP/EPDM
Information provided by Polykemi AB
Mold Temperature 20.0 - 60.0 °C
68.0 - 140 °F
Polykemi AB POLYelast TPE R44 Thermoplastic Elastomer
Information provided by Polykemi AB
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Polykemi AB POLYelast TPE Z606 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
Mold Temperature 20.0 - 60.0 °C
68.0 - 140 °F
Injection Molding
Polimeri Europa Edistir ICE S 800/N Polystyrene  (discontinued **)
Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular t..
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Termopol Termoton® V5GA1090A TPV Compound
Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;..
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Injection
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop..
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Injection
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
Mold Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Gromax 1172LL TPE
1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac..
Mold Temperature 20.0 °C
68.0 °F
Recommended
MBA Polymers HDPE 1107 E Post-consumer recycled fractional melt high density polyethylene
Available in standard black.Information provided by MBA Polymers.
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
LATI Latistat 45/7-02 HDPE
Dissipative product based on High density polyethylene (HD-PE). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
SK Chemicals SKYTHANE® S185A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
SK Chemicals SKYTHANE® S198A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
SK Chemicals SKYTHANE® S392A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
SK Chemicals SKYTHANE® S395A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer
SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Covestro Desmopan® 3385A Polyurethane
Extrusion- and injection molding gradegood wear resistanceshort cycle timeshigh melt stabilityApplicationhard - soft systemsHosesnon-reinforcedProfilesInjection molded engineering partsPreprocessing..
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Covestro Desmopan® 481 Polyurethane
injection molding gradefree from plasticizersgrease and oil-resistantlow compression sethigh elasticitygood heat resistanceEasy releaseApplicationRoller coatingSealsmembranesAutomotive engineeringPr..
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Covestro Desmopan® DP 1080A Polyurethane
injection molding gradefree from plasticizershard - soft systemsTechnical partsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covest..
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Covestro Desmopan® DP 2792A Polyurethane
Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Covestro Desmopan® DP 9665DU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPneuma..
Mold Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Eurotec® Tecolen® HP10 GR20 NL PPCP, 20% glass fiber reinforced, natural
Information provided by Eurotec®
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
BASF Elastollan B 60 D TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup..
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
BASF Elastollan B 80 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup..
Mold Temperature 20.0 - 80.0 °C
68.0 - 176 °F
Arkema Group Rilsan® Clear G350 Polyamide
Rilsan® Clear G350 is a high performance transparent polyamide. This grade has been specially designed for injection molding applications, ideally suited for optics as high end eyewear frames.Infor..
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
BASF Elastollan B 85 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup..
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
BASF Elastollan C 85 A HPM TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c..
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Wacker Silicones Geniomer® 60 Silicone TPE
SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase..
Mold Temperature 20.0 - 82.2 °C
68.0 - 180 °F
Average value: 41.4 °C Grade Count:14
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and ..
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Termopol Termoton® K2GA2060A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..