Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 100 Thermoset Polyester, GP BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1603 Multi-purpose grade BMC 1603 is a multi-purpose, moderate strength, low cost material that is suitable for injection, compression and transfer molding. UL® recognized. This material was formerly known as Glastic® 160.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 2270 Mineral Filled, Glass Reinforced Polyester BMC 2270 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a general purpose material with medium impact strength a.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 404 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 404 is a high strength, low shrink, glass reinforced polyester molding compound that meets Ford Specification ESF-M3D121-A. BMC 404 has excellent electrical properties and creep resistance. It c.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 501E Mineral Filled, Glass Reinforced Polyester BMC 501E molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a product with good overall electrical properties, flame.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 5209 Mineral Filled, Glass Reinforced Polyester BMC 5209 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 610 - SP Mineral Filled, Glass Reinforced Polyester Compound, with UV Stabilizer BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 615 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 615 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ext.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 680 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression and stuffer injection molding It is characterized by good moldability, very high impa.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 685 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, oil .. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant BMC 800 compounds are UL rated 94V0/5V. These compounds exhibit excellent strength, corrosion and weather resistant properties. As with all other BMCI compounds, this Series can be supplied in logs,.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 880 Medium Strength Molding Compound BMC 880 is a medium strength, low shrink molding compound designed for outdoor applications. This material is UL Listed 94-V0/5V and is UL approved for outdoor use. It can be supplied in bulk or ext.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 901 Encapsulating Grade Molding Compound BMC 901 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 902 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 902 is a medium strength, high flow molding compound that meets Ford Specification ESFM3D114- A. BMC 902 has excellent electrical properties and creep resistance. It can be pigmented in a wide r.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1401 Encapsulating Material, Electrical Grade BMC 1401 is an electrical grade of encapsulating material characterized by a balance of soft flow and cure rate to ensure complete and proper encapsulation without voiding. Generally too soft for co.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1410 Electrical Grade BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1901 Mineral Filled Alkyd BMC 1901 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression transfer molding. It is a general purpose with medium impact strength and good overall e.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 200 Thermoset Polyester, Electrical Grade BMC 200 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, bobbins, electrical conne.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 5209-12940 Mineral Filled, Glass Reinforced Polyester BMC 5209-12940 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 5592 Arc, Track, and Weather Resistant Polyester BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame re.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by good moldability high impact st.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 8005 Polyester Molding Compound |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 945 Conductive Grade Bulk Molding Compound BMC 945 is an ESD level Conductive grade of Bulk Molding Compound and is suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reacti.. |