Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 21.0 - 38.0 °C | 69.8 - 100 °F | |
NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equip.. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Eastar GN125 Copolyester, Natural
(discontinued **) Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co.. |
|||
Mold Temperature | 15.0 - 38.0 °C | 59.0 - 100 °F | Average value: 22.9 °C Grade Count:11 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Drystar 0325 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Drystar 0603 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Drystar 0827 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman DuraStar MN611 Polymer, Natural Durastar Polymer MN611 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Eastar 5011 Copolyester Eastar Copolyester 5011 is a glycol modified polyethylene terephthalate(PET). The modification is made by adding a second glycol, cyclohexanedimethanol (CHDM) during the polymerization stages. The s.. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Eastar DN010 Copolyester Eastar Copolyester DN010 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN010 contains no mold release.Applications.. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Eastar DN011 Copolyester Eastar Copolyester DN011 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN011 contains a mold release.Applications/.. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Eastar DN114 Copolyester, Natural Applications:LightingProduct Description: Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage. DN1.. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Eastar GN119 Copolyester Applications:Personal care and CosmeticsProduct Description: Eastar GN119 Copolyester is a low-I.V. PETG, for sale only in Asia as a high-flow formulation. This product has been GREENGUARD INDOOR .. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Eastar GN120 Copolyester Applications:AppliancesConsumer electronicsPersonal care and cosmeticsStationary suppliesKey Attributes:High clarity and transparencyHigh flow copolyesterToughProduct Description: Eastar GN120 Cop.. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Eastar MN006 Copolyester Eastar Copolyester MN006 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester MN006 contains a mold release.Applications/.. |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Eastar MN200 Copolyester Eastar Copolyester MN200 is an amorphous copolyester with excellent flow characteristics as well as radiation resistance and chemical resistance.Applications/UsesMedical |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Eastar MN210 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates.Applications/UsesMedical |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Eastar MN211 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. MN211 contains a mold release.Application.. |
|||
Mold Temperature | 10.0 - 38.0 °C | 50.0 - 100 °F | |
Ecomass® 4450CI86 Carbonyl Iron Filled Polypropylene Nontoxic alternative to Lead (Pb), for shielding applicationsHigh Specific GravityCarbonyl Iron Filled Polypropylene Random Co-PolymerInformation provided by Technical Polymers |
|||
Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
Eastman Eastar GN046 Copolyester, Natural Eastar Copolyester GN046 is a very high melt strength copolyester targeted for extrusion blow molding applications. Blow molding of large parts (up to several pounds) are possible with this material.. |