| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
|
SABIC MG200024 Linear Low Density Polyethylene for Compounding
Product Description: MG200024 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution primarily suitable for compounding. It is in the powder form designed to give g..
|
|||
| Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
|
SABIC PP 413MNK45 Polypropylene Impact Copolymer for Injection Molding
Product Description: PP 413MNK45 is a controlled rheology PP grade with a very high fluidity. It is provided with an antistatic package & nucleating agent and is especially developed for producing..
|
|||
| Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
|
SABIC PP 513MN40 Polypropylene Impact Copolymer for Injection Molding
Product Description: PP 513MN40 is a controlled rheology PP grade of narrow molecular weight distribution. It contains an antistatic agent and is especially developed for producing injection molde..
|
|||
| Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
|
SABIC PP 5702P Polypropylene Homopolymer for Injection Molding
Product Description: PP 5702P is specially developed for rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the products.Typical..
|
|||
| Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
|
SABIC PP 5703P Polypropylene Homopolymer for Injection Molding
Product Description: PP 5702P is specially developed for producing rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the produc..
|
|||
| Mold Temperature | 15.0 - 15.0 °C | 59.0 - 59.0 °F | (close to) |
|
Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding
The Trithene® SX 7010 resin is a medium molecular weight, low-density polyethylene (LDPE) which allows the production of flasks with an adequate combination of mechanical and impact strength, flexi..
|
|||
| Mold Temperature | 15.0 - 95.6 °C | 59.0 - 204 °F | Average value: 39.6 °C Grade Count:42 |
|
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
|
|||
| Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
|
Eastman Eastar GN002 Copolyester, Natural
(discontinued **)
Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha..
|
|||
| Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
|
Eastman Eastar GN102 Copolyester
(discontinued **)
Eastar GN102 copolyester is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet inhibitor and mold release. Eastar GN102 copolyester will not crystallize and thus offers ..
|
|||
| Mold Temperature | 15.0 - 38.0 °C | 59.0 - 100 °F | Average value: 22.9 °C Grade Count:11 |
|
Overview of materials for PCTG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
|
|||
| Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
|
SABIC M200056 High Density Polyethylene for Injection Molding
Product Description: M200056 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow..
|
|||
| Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
|
SABIC PP 674K Polypropylene Copolymer for Injection Molding
Product Description: PP 674K is specially developed for producing injection molded & ISBM articles with high clarity and also has better impact properties than homo PP counterparts.PP 674K has the ..
|
|||
| Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
|
Inno-Comp INNOPOL® CS 2-2130 30% Talc Filled Polypropylene Copolymer
INNOPOL® CS 2-2130 is a 30 % talc-filled polypropylene compound /PP-B TD30 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-2130 is recommended for produci..
|
|||
| Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
|
Inno-Comp INNOPOL® CS 2-5830 SA 30% Glass Filled Polypropylene Copolymer
INNOPOL® CS 2-5830 SA is a 30 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-5830 SA is recommended for p..
|
|||
| Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
|
Inno-Comp INNOPOL® CS 3-8000 FR Flame Retardant Polypropylene Blend
INNOPOL® CS 3-8000 FR is a flame retarded polypropylene compound based on a specific blend of polypropylene homo polymer and copolymer. This grade is available in natural and custom colored form...
|
|||
| Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | |
|
Inno-Comp INNOPOL® CS 1-2120 AP 20% Talc Filled Polypropylene Homopolymer
INNOPOL CS 1-2120 AP is a 20 % talc filled compound based on polypropylene homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 1-2120 AP is recommended especially..
|
|||
| Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
|
LATI Latigea B01 L/07 Bio-Polymer
Bio-Polymer (PLA, PHB, ...) based compound. Wood flour. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p..
|
|||
| Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
|
Borealis HH315MO Polypropylene
HH315MO is a polypropylene homopolymer intended for injection molding. Its high melt flow makes it especially suitable for products with long flow length. This grade is designed for high-speed injec..
|
|||
| Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
|
Borealis RJ900MO Polypropylene Random Copolymer
RJ900MO is a polypropylene random copolymer with high melt flow and good transparency. Products originating from this grade have excellent transparency and gloss, and good balance of stiffness and ..
|
|||
| Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
|
Eastman Drystar 0113 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
|
|||
| Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
|
Eastman DuraStar DS1000 Polymer, Natural
Durastar DS1000 polymer has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to aromatic oils often causes c..
|
|||
| Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
|
Eastman DuraStar DS1110UVI Polymer, Natural
Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li..
|
|||
| Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
|
Eastman DuraStar DS2000 Polymer, Natural
Durastar DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has ver..
|
|||
| Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
|
Eastman DuraStar MN620 Polymer, Natural
Applications:Blood therapyDrug deliveryIV componentsMedicalSurgical instrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAProduct Description: DuraStar Poly..
|
|||
| Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
|
Eastman Eastar AN001 Copolyester, Natural
Eastar AN001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca..
|
|||
| Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
|
Eastman Eastar MN004 Copolyester
Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl..
|
|||
| Mold Temperature | 15.0 - 50.0 °C | 59.0 - 122 °F | EBM |
|
Eastman Tritan TX1801 Copolyester, Natural
Applications:Consumer and durable goodsExtrusion blow moldingInjection stretch blow moldingKey Attributes:Ease of processingExcellent clarityExcellent Hydrolytic stabilityGood chemical resistanceGoo..
|
|||
| Mold Temperature | 15.0 - 95.0 °C | 59.0 - 203 °F | |
|
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded
Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb..
|
|||
| Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
|
LATI Latimass 37 B01-01 D025 Bio-Polymer
Specific density compound based on Bio-Polymer (PLA, PHB, ...). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
|
|||
| Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
|
LATI Latigea B01 I6 Bio-Polymer
Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p...
|
|||