Polymer Property : Rear Barrel Temperature = 195 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Injection Molding
Ineos ABS Lustran® 266 ABS, Transparent Grade
Lustran® ABS 266 resin is a clear injection molding grade of ABS (acrylonitrile butadiene styrene). This transparent, general-purpose grade provides clarity and toughness with ease of processing...
Rear Barrel Temperature 195 - 205 °C
383 - 401 °F
Huntsman AVALON® 90 AK Thermoplastic Polyurethane
Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har..
Rear Barrel Temperature 195 - 205 °C
383 - 401 °F
Huntsman AVALON® 90 AKU Thermoplastic Polyurethane
Introduction: AVALON 90 AKU is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same ha..
Rear Barrel Temperature 195 °C
383 °F
Injection
Alliance Polymers Zythane™ 4050D Thermoplastic Polyurethane Elastomer
Zythane™ 4050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Rear Barrel Temperature 195 °C
383 °F
Injection
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer
Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Rear Barrel Temperature 195 °C
383 °F
Injection
Alliance Polymers Zythane™ 6050D Thermoplastic Polyurethane Elastomer
Zythane™ 6050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Rear Barrel Temperature 195 °C
383 °F
Injection
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer
Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Rear Barrel Temperature 195 °C
383 °F
Injection
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Rear Barrel Temperature 195 - 220 °C
383 - 428 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..