| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber |
| Manufacturer | Arlon |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Arlon CP-510R Silicone Rubber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.35 g/cc | 1.35 g/cc | Arlon SQA-TMS-024 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 60 | 60 | ASTM D2240 |
| Tensile Strength, Ultimate | 5.52 MPa | 800 psi | ASTM D412 |
| Elongation at Break | 225 % | 225 % | ASTM D412 |
| Tear Strength | 15.8 kN/m | 90.0 pli | Die B; silicone property; ASTM D624 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
| Minimum Service Temperature, Air | -56.7 °C | -70.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 120 min @Temperature 204 °C |
2.00 hour @Temperature 400 °F |
|
| 15.0 min @Pressure 0.345 MPa, Temperature 121 °C |
0.250 hour @Pressure 50.0 psi, Temperature 250 °F |
||
| Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Red |