| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
| Spiral Flow | 88.9 cm | 35.0 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 75 | 75 | ASTM D2240 |
| Tensile Strength, Yield | 37.9 MPa | 5500 psi | Type I, 51 mm/min; ASTM D638 |
| Elongation at Break | 60 % | 60 % | Type I, 51 mm/min; ASTM D638 |
| Tensile Modulus | 2.28 GPa | 331 ksi | Type I, 51 mm/min; ASTM D638 |
| Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
| Flexural Modulus | 2.28 GPa | 331 ksi | ASTM D790 |
| Izod Impact, Notched | 2.10 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
3.93 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
| 5.90 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
11.1 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A | |
| 7.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
14.1 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 71.1 °C @Thickness 6.35 mm |
160 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
| 77.2 °C @Thickness 6.35 mm |
171 °F @Thickness 0.250 in |
Annealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C @Thickness 6.35 mm |
158 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
| 72.8 °C @Thickness 6.35 mm |
163 °F @Thickness 0.250 in |
Annealed; ASTM D648 | |
| UL RTI, Electrical | 90.0 °C | 194 °F | UL 746 |
| UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746 |
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746 |
| Flammability, UL94 | V-0 @Thickness 1.40 mm |
V-0 @Thickness 0.0551 in |
ALL; UL 94 |
| V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
All Colors | |
| 5VB @Thickness 1.91 mm |
5VB @Thickness 0.0752 in |
All Colors | |
| 5VB @Thickness 1.40 mm |
5VB @Thickness 0.0551 in |
ALL; UL 94 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 199 - 210 °C | 390 - 410 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | General Purpose | |
| High Flow | ||
| Low Temperature Impact Resistance | ||
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Appliances | |
| Business Equipment | ||
| Construction Applications | ||
| Electrical/Electronic Applications | ||
| General Purpose | ||
| Telecommunications |