| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Cycolac® MG29 ABS (Asia Pacific)
Super high impact ABS. Good low temperature toughness. High gloss.
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Cycolac® MG38 ABS
Very high impact ABS. Toughness/rigidity. Good fatigue resistance.
|
|||
| Arc Resistance | 110 - 180 sec | 110 - 180 sec | Average value: 130 sec Grade Count:4 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | UL-746A rating 5 (120-180 sec) |
|
Shell Carilon® DB6F5G40 Polyketone, Flame-Retarded (V-0), 20% Glass-Reinforced Injection Molding Grade
(disco
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F5G40 is a flame-retarded, 20 percent glass-fiber-reinforced, injection molding grade with mecha..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS
High impact and ductility at 73F (23C) and -20F (-29C).
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS (Asia Pacific)
PC+ABS, excellent flow/impact/high heat resistance. Suitable for thin wall application. Low temperature ductility (-20F). For automotive, appliance and electrical components.
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
LG Chemical Lupox® GP2300R PBT+GF30%
Description: Injection Molding, PBT+GF30%, Anti-HydrolysisApplication: E&E (Speed Nut & Body)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
LG Chemical Lupoy 1301V-7 Polycarbonate Resin
Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | UL Rating PLC 5 (120-180 sec) |
|
LG Chemical MI-750 MIPS
Medium impact
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin
Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC
LNP* Lubricomp* Lexan_WR2210 compound is an alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121.
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
|
SABIC Innovative Plastics Ultem 1000FV PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics ULTEM 1000R PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing.
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics ULTEM 1000RV PEI
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
|
SABIC Innovative Plastics Ultem 1000V PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in ..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics ULTEM 1010F PEI
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer b..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
|
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
|
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Valox® 4521 PBT (Asia Pacific)
19.5% glass reinforced PBT. High flow, flame retardant.
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Valox® DR51 PBT
15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Xenoy® 1731 PBT+PC
Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Xenoy® 5220U PBT+PC
Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance.
|
|||
| Arc Resistance |
120
-
180
sec @Thickness 3.00 mm |
120
-
180
sec @Thickness 0.118 in |
UL Rating PLC 5 (120-180 sec) |
|
Covestro Bayblend® T 85 MN Polycarbonate/ABS Blend
High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 ..
|
|||
| Arc Resistance |
120
-
180
sec @Thickness 3.00 mm |
120
-
180
sec @Thickness 0.118 in |
UL 746A |
|
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded
Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro..
|
|||
| Arc Resistance |
120
-
180
sec @Thickness 3.00 mm |
120
-
180
sec @Thickness 0.118 in |
UL Rating PLC 5 (120-180 sec) |
|
Covestro Apec® DP9-9353 High-Heat Polycarbonate, UV Stabilized
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000A PC (Europe-Africa-Middle East)
LNP* Thermocomp* Lexan_LGN2000A compound is a 20% glass reinforced PC, high flow. UL rated V-0. Consumer Electronics applications.
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
LG Chemical HIPS MI750 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer..
|
|||