| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Cycolac® MG29 ABS
Super high impact ABS. Good low temperature toughness. High gloss.
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
|
SABIC Innovative Plastics Lexan® 133 PC (Asia Pacific)
Nonhalogenated. 3.5 MFR. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 117 sec Grade Count:14 |
|
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
|
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 107 sec Grade Count:3 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe..
|
|||
| Arc Resistance | 80.0 - 180 sec | 80.0 - 180 sec | Average value: 103 sec Grade Count:3 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
|
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 105 sec Grade Count:8 |
|
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled
Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications.
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
Idemitsu Kosan Xarec® WA 212LG SPS, 30% Glass Filled |
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
LG Chemical KEYFLEX BT 1055D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
LG Chemical Lupox® GP1000S PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
LG Chemical Lupox® GP1000W PBT
Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
LG Chemical Lupoy 1302-05 Polycarbonate Resin
Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
LG Chemical 90HR SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Battery Case, Light CoverCAS No. 9003-54-7Information provided by LG Chemical
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | UL Rating PLC 5 (120-180 sec) |
|
LG Chemical 92HR SAN Resin
Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
|
LG Chemical Lupoy 1303-15 Polycarbonate Resin
Description: LUPOY PC 1303-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
|
SABIC Innovative Plastics Ultem 1000FV PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
|
SABIC Innovative Plastics Ultem 1000FV PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
|
SABIC Innovative Plastics Ultem 1000V PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in ..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
|
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
|
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
|
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics ULTEM 1110F PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant, NSF 51 listing. UL94 V0 and 5VA listing. Effective June 2007, this grade will no longer be supported w..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
|
SABIC Innovative Plastics Ultem 2412EPR PEI
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics ULTEM CRS5111 PEI
10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing.
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
|
SABIC Innovative Plastics Ultem CRS5211 PEI (Asia Pacific)
20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Thi..
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Valox® 364 PBT+PC
Designed for outdoor telecommunications enclosure applications.
|
|||
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
|
SABIC Innovative Plastics Valox® 4521 PBT (Asia Pacific)
19.5% glass reinforced PBT. High flow, flame retardant.
|
|||
| Arc Resistance |
120
-
180
sec <br>@Thickness 3.00 mm
|
120
-
180
sec <br>@Thickness 0.118 in
|
UL 746A |
|
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded
Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb..
|
|||
| Arc Resistance | 60.0 - 180 sec | 60.0 - 180 sec | Average value: 124 sec Grade Count:6 |
|
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
|
|||