Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 2.00e+14 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
ASTM D257
Rogers Corporation TMM® TMM101 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
DC, 65% RH; ASTM D257
Arkema Group Kynar Flex® 2900 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
DC, 65% RH; ASTM D257
Arkema Group Kynar Flex® 2950 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
ASTM D257
Techmer ES Elastoblend® PA6/6 IM L W Nylon 66
Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc...
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
ASTM D257
Unitika P-5001 Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
ASTM D257
Westlake Plastics Ardel® Polyarylate
Stock shapes extruded from Ardel resin are specifically formulated to endure the damaging effects of UV light. When exposed to UV light, this unique material undergoes a molecular rearrangement res..
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
Tra-Con Tra-Bond FDA15 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA-15 is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Adminis..
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
ASTM D257
Unitika L-8005
Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd.
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
Dow Corning HV 1660/65 LIGHT GRAY SILICONE RUBBER KP
65 Shore hardness high consistency silicone rubber with excellent tracking and erosion resistance, excellent wet electrial properties,high voltage insulation applications.Information provided by Dow..
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
Dow Corning SILASTIC® HV 1666/65 GRAY SILICONE RUBBER
65 Durometer, gray, peroxide cure, high voltage grade Silicone Rubber Compound for manufacturing High Voltage insulators weather shed insulators or surge arrestors. Superior wet electrical propertie..
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
cond; IEC 60093
DSM EcoPaXX® Q-X07209 PA410-I-GF40
% Glass Reinforced, Impact Modified
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
dry; IEC 60093
DSM Novamid® 1013G45 1 NA PA6-GF45
45% Glass Reinforced, Injection Molding
Volume Resistivity <= 2.00e+14 ohm-cm
<= 2.00e+14 ohm-cm
Cytec (Conap) FR-1271 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
ASTM D257
Fainplast Compounds Hax™ HF 4024 Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Insulation and sheathing, improved processabilityInformation provided by Fainplast Compo..
Volume Resistivity 2.00e+14 ohm-cm

@Temperature 23.0 °C
2.00e+14 ohm-cm

@Temperature 73.4 °F
ASTM D257
Fainplast Compounds KL 84/1 Flexible PVC, Insulation for High Temperatures Lead Free
General purposes flame retardant
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
C96/35/90; IPC TM-650 2.5.17.1
Arlon 85NT Polyimide Nonwoven Aramid Laminate and Prepreg
85NT is a pure polyimide laminate and prepreg system (Tg = 250°C), reinforced with a non-woven aramid substrate. This system combines the high-reliability features of polyimide (improved PTH relia..
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
Atom Adhesives AA-BOND FDA15 Epoxy Adhesive
AA-BOND FDA15 is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Administr..
Volume Resistivity 2.00e+14 ohm-cm

@Temperature 20.0 °C
2.00e+14 ohm-cm

@Temperature 68.0 °F
65% RH; ASTM D257
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Volume Resistivity 2.00e+14 ohm-cm

@Temperature 20.0 °C
2.00e+14 ohm-cm

@Temperature 68.0 °F
65% RH; ASTM D257
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Volume Resistivity 2.00e+14 ohm-cm

@Temperature 20.0 °C
2.00e+14 ohm-cm

@Temperature 68.0 °F
65% RH; ASTM D257
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Volume Resistivity 2.00e+14 ohm-cm

@Temperature 20.0 °C
2.00e+14 ohm-cm

@Temperature 68.0 °F
65% RH; ASTM D257
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
Volume Resistivity 2.00e+14 ohm-cm

@Temperature 20.0 °C
2.00e+14 ohm-cm

@Temperature 68.0 °F
65% RH; ASTM D257
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Volume Resistivity 2.00e+14 ohm-cm

@Temperature 20.0 °C
2.00e+14 ohm-cm

@Temperature 68.0 °F
65% RH; ASTM D257
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
Volume Resistivity 2.00e+14 ohm-cm

@Temperature 20.0 °C
2.00e+14 ohm-cm

@Temperature 68.0 °F
65% RH; ASTM D257
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
50% RH; ASTM D-257
Axiall 17940 Wire & Cable Flexible PVC
THW insulation compound. Also suitable for 105C applications in 3/64 and larger sizes. UL recognized component for THW. Oil resistant I, VW-1 rated.Information provided by Georgia GulfGeorgia Gul..
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
50% RH, 500V; ASTM D257
ALM PA-615-GS Filled Nylon 12 Prototyping Polymer
50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially ..
Copyright © lookpolymers.com All Rights Reserved