ExxonMobil EXACT™ 0210 Ethylene-based Plastomer for Multilayer Film Applications |
Film |
EXACT™
|
ExxonMobil EXACT™ 0230 Plastomer for Multilayer Film Applications |
Film |
EXACT™
|
ExxonMobil EXACT™ 3024 Plastomer for Cast Film Applications |
Film |
EXACT™
|
ExxonMobil EXACT™ 3027 Plastomer for Cast Film Applications |
Thermoplastic Olefinic Elastomer (TPO), Film Grade |
EXACT™
|
ExxonMobil Exact™ 3040 Cast Ethylene-based Plastomer Resin |
Elastomer, TPE |
EXACT™
|
ExxonMobil EXACT™ 3040 Plastomer for Extrusion Coating Applications |
Film |
EXACT™
|
ExxonMobil EXACT™ 3128 Plastomer for Blown Film Applications |
Film |
EXACT™
|
ExxonMobil EXACT™ 3131 Plastomer for Cast Film Applications |
Film |
EXACT™
|
ExxonMobil EXACT™ 3132 Plastomer for Blown Film Applications |
Film |
EXACT™
|
ExxonMobil EXACT™ 3139 Plastomer for Cast Film Applications |
Film |
EXACT™
|
ExxonMobil EXACT™ 4049 Plastomer for Elastic Film and Elastic Film Blends |
Film |
EXACT™
|
ExxonMobil EXACT™ 4053 Cast Plastomer |
Polyethylene (PE) |
EXACT™
|
ExxonMobil EXACT™ 4053 Plastomer for Film Applications |
Thermoplastic Olefinic Elastomer (TPO), Film Grade |
EXACT™
|
ExxonMobil EXACT™ 4056 Plastomer for Film Blends and Blown Film Applications |
Film |
EXACT™
|
ExxonMobil EXACT™ 4150 Plastomer |
Thermoplastic Olefinic Elastomer (TPO), Film Grade |
EXACT™
|
ExxonMobil Exact™ 4151 Ethylene-based Plastomer Resin |
Elastomer, TPE |
EXACT™
|
ExxonMobil EXACT™ 4151 Plastomer for Cast Film |
Film |
EXACT™
|
ExxonMobil Exact™ 4160 Series Ethylene-based Plastomer Resin |
Elastomer, TPE |
EXACT™
|
ExxonMobil EXACT™ 8210 Plastomer for Multilayer Film Applications |
Film |
EXACT™
|
ExxonMobil EXACT™ 8230 Plastomer for Polymer Modification |
Additive/Filler for Polymer |
EXACT™
|
ExxonMobil Exact™ 9061 Ethylene-based Plastomer Resin |
Elastomer, TPE |
EXACT™
|
ExxonMobil Exact™ 9071 Ethylene-based Plastomer Resin |
Elastomer, TPE |
EXACT™
|
ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin |
Elastomer, TPE |
EXACT™
|
ExxonMobil Exact™ 9371 Ethylene-based Plastomer Resin |
Elastomer, TPE |
EXACT™
|
ExxonMobil EXXELOR™ PO 1020 Maleic anhydride functionalized polypropylene |
Additive/Filler for Polymer |
EXXELOR™
|
ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Geolast®
|
ExxonMobil Santoprene® 101-45W255 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 101-55W255 Thermoplastic Vulcanizate |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-50E500 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-50M100 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-55W241 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-58W175 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-60M200 Thermoplastic Vulcanizate - UV Resistant |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-62M100 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-65B200 Thermoplastic Vulcanizate - UV Resistant |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-67W175 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-70B230 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-70M350 Thermoplastic Vulcanizate - UV Resistant |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-73W175 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-75M100 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-75M200 Thermoplastic Vulcanizate - UV Resistant |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-79W233 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-80B230 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-80W175 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-85M100 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 123-40 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 123-50W175 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 123-52W242 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 151-70W256 Thermoplastic Vulcanizate - Flame Retardant |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 181-57W180 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 201-55W255 Thermoplastic Vulcanizate |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 201-80 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 241-55 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 241-73W236 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 241-80W236 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 251-70W232 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 251-80W232 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 251-85W232 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 251-92W232 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 271-55 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 271-64 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 271-80 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 271-87 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 291-60B150 Thermoplastic Vulcanizate |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 291-75B150 Thermoplastic Vulcanizate |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 691-65W175 Thermoplastic Vulcanizate |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 691-73W175 Thermoplastic Vulcanizate |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8201-80HT Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8211-55B100 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8211-75 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8211-85M350 Thermoplastic Vulcanizate |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8221-55M300 Thermoplastic Vulcanizate - UV Resistant |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8221-65M300 Thermoplastic Vulcanizate - UV Resistant |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8221-75M300 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8221-85M300 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8223-30M300 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer |
Thermoplastic Vulcanizate Elastomer (TPV) |
Santoprene®
|