ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Geolast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A hard, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applications. This grade of Geolast TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Recyclable. Designed for improved fluid resistance.Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
Air at 257°F, 168 hr; ASTM D573
84
84
.12 in; ASTM D2240
Tensile Strength at Break 7.4967 MPa
1087.3 psi
257°F, 70 hr in IRM 903 Oil; ASTM D471
9.03 MPa
1310 psi
Across Flow; ASTM D412
10.387 MPa
1506.5 psi
Air at 257°F, 168 hr; ASTM D573
Tensile Strength, Ultimate 5.03 MPa
730 psi
Across Flow; ASTM D412
Elongation at Break 227.7 %
227.7 %
257°F, 70 hr in IRM 903 Oil; ASTM D471
244.2 %
244.2 %
Air at 257°F, 168 hr; ASTM D573
330 %
330 %
Across Flow; ASTM D412
Tear Strength 34.0 kN/m
194 pli
73°C, Die C; ASTM D624
Compression Set 39 %
39 %
158°F, 22 hr; ASTM D395
50 %
50 %
257°F, 70 hr; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Melt Temperature <= 102 °C
<= 215 °F
Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 0.48
Color Black
Form Pellets