Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : FiberFil > Category : Polymer Product List

Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
Fiberfil® FPI-15 BK Nylon 6, 15% Glass Reinforced, post industrial Nylon 6
Fiberfil® FPI-33 BK Nylon 6, 33% Glass Reinforced, post industrial Nylon 6
Fiberfil® FV-30 Nylon 6, 30% Glass Reinforced, Heat Stabilized Nylon 6
Fiberfil® FV-31 Nylon 6, 31% Glass Reinforced, Heat Stabilized Nylon 6
Fiberfil® J-60/10 Polypropylene Homopolymer, 10% Glass Reinforced Polypropylene (PP)
Fiberfil® J-60/10/CC/30/E NATL Polypropylene Homopolymer, 10% FiberGlass and 30% Calcium Carbonate Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/10/E Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/10/E/M Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/10/FR Polypropylene Homopolymer, 10% Glass Reinforced, Flame Retardant Polypropylene (PP)
Fiberfil® J-60/15/E Polypropylene Homopolymer, 15% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/20 Polypropylene Homopolymer, 20% Glass Reinforced Polypropylene (PP)
Fiberfil® J-60/20/E Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/20/E/NS Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, NSF listed Polypropylene (PP)
Fiberfil® J-60/20/E4 Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/20/E8 Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/20/FR Polypropylene Homopolymer, 20% Glass Reinforced, Flame Retardant Polypropylene (PP)
Fiberfil® J-60/20/H Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/20/TT/FD WT8381 Polypropylene Homopolymer, 20% Glass Reinforced, FDA compliant Polypropylene (PP)
Fiberfil® J-60/30 Polypropylene Homopolymer, 30% Glass Reinforced Polypropylene (PP)
Fiberfil® J-60/30/E Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow Polypropylene (PP)
Fiberfil® J-60/30/E/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/30/E/NS Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, NSF listed Polypropylene (PP)
Fiberfil® J-60/30/E3 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/30/E4 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/30/E8 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/30/E8/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/30/F Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/30/FR Polypropylene Homopolymer, 30% Glass Fiber Reinforced, Flame Retardant Polypropylene (PP)
Fiberfil® J-60/40 Polypropylene Homopolymer, 40% Glass Reinforced Polypropylene (PP)
Fiberfil® J-60/40/E Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/40/E/EX Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled, high viscosity Polypropylene (PP)
Fiberfil® J-60/40/E8 Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/GB/20 Polypropylene Homopolymer, 20% Glass beads Polypropylene (PP)
Fiberfil® J-68/20/E/SD/HM Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled, with static dissipation Polypropylene (PP)
Fiberfil® J-68/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-69/10/E High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-69/10/E/UV High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled, UV Stabilized Polypropylene (PP)
Fiberfil® J-69/30/E High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-69/30/E/M High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® M-1492 BK223 Polypropylene Homopolymer, Glass Reinforced, mica Filled, Chemically coupled Polypropylene (PP)
Fiberfil® M-1812 Polypropylene Homopolymer, 45% Talc Filled Polypropylene (PP)
Fiberfil® M-2149 Polypropylene Homopolymer, 30% Glass Reinforced Polypropylene (PP)
Fiberfil® M-2271 NAT Nylon 6, 33% Glass Reinforced, post industrial, natural Nylon 6
Fiberfil® M-2450 BK9083 Polypropylene Copolymer, 20% Talc Polypropylene (PP)
Fiberfil® M-2450 Polypropylene Copolymer Polypropylene (PP)
Fiberfil® M-2494 BK Nylon 6, 30% FiberGlass Reinforced, post industrial grade Nylon 6
Fiberfil® M-2500 BK Nylon 6, 15% Glass Reinforced, 25% mineral Filled, post industrial Nylon 6
Fiberfil® PP-60/CC/40 Polypropylene Homopolymer, 40% Calcium Carbonate Polypropylene (PP)
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0 Polypropylene (PP)
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled Polypropylene (PP)
Fiberfil® PP-60/TC/13 BL8860 Polypropylene Homopolymer, 13% Talc Filled Polypropylene (PP)
Fiberfil® PP-60/TC/15/VO/ND Polypropylene Homopolymer, 15% Talc Filled, Flame Retardant Polypropylene (PP)
Fiberfil® PP-60/TC/20 Polypropylene Homopolymer, 20% Talc Filled Polypropylene (PP)
Fiberfil® PP-60/TC/20/FD Polypropylene Homopolymer, 20% Talc Filled, FDA compliant Polypropylene (PP)
Fiberfil® PP-60/TC/20/VO/ND Polypropylene Homopolymer, 20% Talc Filled, Flame Retardant Polypropylene (PP)
Fiberfil® PP-60/TC/24/D/HS Polypropylene Homopolymer, Talc Filled, Heat Stabilized Polypropylene (PP)
Fiberfil® PP-60/TC/30 Polypropylene Homopolymer, 30% Talc Filled Polypropylene (PP)
Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled Polypropylene (PP)
Fiberfil® PP-60/TC/40/OP WT2595 Polypropylene Homopolymer, 40% Talc Filled, high opacity Polypropylene (PP)
Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2 Polypropylene (PP)
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0 Polypropylene (PP)
Fiberfil® PP-60/VO/NH Polypropylene Homopolymer, Flame Retardant, non-halogenated, UL94 V0 Polypropylene (PP)
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Polypropylene (PP)
Fiberfil® PP-61/CC/40 Polypropylene Copolymer, 40% Calcium Carbonate Polypropylene (PP)
Fiberfil® PP-61/TC/20 Polypropylene Copolymer, 20% Talc Polypropylene (PP)
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized Polypropylene (PP)
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Polypropylene (PP)
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0 Polypropylene (PP)
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0 Polypropylene (PP)
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Polypropylene (PP)
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced Polypropylene (PP)
Fiberfil® PP-68/TC/20 Polypropylene Copolymer, 20% Talc Polypropylene (PP)
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Polypropylene (PP)
Fiberfil® J-60/10/E8 Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/15/MI/20 Polypropylene Homopolymer, 35% Glass/mica Reinforced Polypropylene (PP)
Fiberfil® J-60/15/UV/HS Polypropylene Homopolymer, 15% Glass Reinforced, Heat Stabilized, UV Stabilized Polypropylene (PP)
Fiberfil® J-60/20/E/HF Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, improved flow Polypropylene (PP)
Fiberfil® J-60/20/E8/M Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-61/10 Polypropylene Copolymer, 10% Glass Fiber Reinforced Polypropylene (PP)
Fiberfil® J-61/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-61/30/FR Polypropylene Copolymer, 30% Glass Reinforced, Flame Retardant Polypropylene (PP)
Fiberfil® J-62/30/E8 Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-68/10/E Polypropylene Copolymer, 10% Glass Fiber Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-68/20/E/SD Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled, with static dissipation Polypropylene (PP)
Fiberfil® J-68/25/E/SD Polypropylene Copolymer, 25% Glass Fiber Reinforced, Chemically coupled, with static dissipation Polypropylene (PP)
Fiberfil® J-69/20/E High performance polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-69/40/E High performance polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® M-2501 BK Nylon 66, 40% mineral Filled, post industrial Nylon 66
Fiberfil® PP-15/T/10/20 Polypropylene Homopolymer, 22% Talc Filled Polypropylene (PP)
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate Polypropylene (PP)
Fiberfil® PP-60/CC/30 Polypropylene Homopolymer, 30% Calcium Carbonate Polypropylene (PP)
Fiberfil® J-62/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-60/30/E5 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-68/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled Polypropylene (PP)
Fiberfil® J-68/30/E/UV Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled, UV Stabilized Polypropylene (PP)
Copyright © lookpolymers.com All Rights Reserved