| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.970 g/cc | 0.970 g/cc | ASTM D792 |
| Water Absorption | 0.030 % | 0.030 % | 24 hr; ASTM D570 |
| Linear Mold Shrinkage | 0.0060 cm/cm @Thickness 6.35 mm |
0.0060 in/in @Thickness 0.250 in |
ASTM D955 |
| 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
ASTM D955 | |
| Melt Flow | 8.0 g/10 min | 8.0 g/10 min | 230/2.16 (typical); ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 100 - 110 | 100 - 110 | ASTM D785 |
| Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
| Elongation at Yield | 4.5 % | 4.5 % | ASTM D638 |
| Tensile Modulus | 3.03 GPa | 440 ksi | ASTM D638 |
| Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
| Flexural Modulus | 2.69 GPa | 390 ksi | Tangent; ASTM D790 |
| Izod Impact, Notched | 0.427 J/cm @Thickness 3.17 mm |
0.800 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 149 °C | 300 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 138 °C | 280 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
| Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
| Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
| Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
| Melt Temperature | 199 - 232 °C | 390 - 450 °F | |
| Mold Temperature | 32.2 - 71.1 °C | 90.0 - 160 °F | |
| Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
| Dry Time | 2 hour | 2 hour | Drying not normally required |
| Moisture Content | <= 0.20 % | <= 0.20 % | recommended for molding |
| Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi |