Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : LyondellBasell > Category : Thermoplastic Product List

Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
LyondellBasell Lupolen® 2012 D SW 413 LDPE Low Density Polyethylene (LDPE), Wire/Cable Grade Lupolen®
LyondellBasell Lupolen® 2210 H SK LDPE Low Density Polyethylene (LDPE), Wire/Cable Grade Lupolen®
LyondellBasell Lupolen® 2410 T LDPE, Injection Molding Grade Low Density Polyethylene (LDPE), Molded Lupolen®
LyondellBasell Lupolen® 2420 F LDPE Low Density Polyethylene (LDPE), Molded Lupolen®
LyondellBasell Lupolen® 2420 H LDPE, Film Grade Low Density Polyethylene (LDPE), Film Grade Lupolen®
LyondellBasell Lupolen® 2420 K LDPE, Film Grade Low Density Polyethylene (LDPE), Film Grade Lupolen®
LyondellBasell Lupolen® 2425 K LDPE, Film Grade Low Density Polyethylene (LDPE), Film Grade Lupolen®
LyondellBasell Lupolen® 2426 F LDPE, Film Grade Low Density Polyethylene (LDPE), Film Grade Lupolen®
LyondellBasell Lupolen® 2441 D LDPE, Film Grade Low Density Polyethylene (LDPE), Film Grade Lupolen®
LyondellBasell Lupolen® 2452 D SW 413 LDPE Low Density Polyethylene (LDPE), Wire/Cable Grade Lupolen®
LyondellBasell Lupolen® 3010 K LDPE, Injection Molding Grade Low Density Polyethylene (LDPE), Molded Lupolen®
LyondellBasell Lupolen® 3020 D LDPE Low Density Polyethylene (LDPE), Molded Lupolen®
LyondellBasell Lupolen® 3020 F LDPE Low Density Polyethylene (LDPE), Molded Lupolen®
LyondellBasell Lupolen® 3020 H LDPE, Film Grade Low Density Polyethylene (LDPE), Film Grade Lupolen®
LyondellBasell Lupolen® 3020 K LDPE, Film Grade Low Density Polyethylene (LDPE), Film Grade Lupolen®
LyondellBasell Lupolen® 3024 H LDPE, Film Grade Low Density Polyethylene (LDPE), Film Grade Lupolen®
LyondellBasell Lupolen® 3025 K LDPE, Film Grade Low Density Polyethylene (LDPE), Film Grade Lupolen®
LyondellBasell Lupolen® 3026 F LDPE, Film Grade Low Density Polyethylene (LDPE), Film Grade Lupolen®
LyondellBasell Lupolen® 3032 D LDPE Low Density Polyethylene (LDPE), Wire/Cable Grade Lupolen®
LyondellBasell Lupolen® 3040 D LDPE, Film Grade Low Density Polyethylene (LDPE), Film Grade Lupolen®
LyondellBasell Lupolen® 3220 K LDPE, Film Grade Low Density Polyethylene (LDPE), Film Grade Lupolen®
LyondellBasell Lupolen® 3226 K LDPE, Film Grade Low Density Polyethylene (LDPE), Film Grade Lupolen®
LyondellBasell Lupolen® 3412 D LDPE Low Density Polyethylene (LDPE), Wire/Cable Grade Lupolen®
LyondellBasell Lupolen® 3652 D SW 00413 MDPE Medium Density Polyethylene (MDPE), Molded Lupolen®
LyondellBasell Lupolen® 3821 D MDPE Medium Density Polyethylene (MDPE), Molded Lupolen®
LyondellBasell Lupolen® 3822 D GB 00350 MDPE Medium Density Polyethylene (MDPE), Molded Lupolen®
LyondellBasell Lupolen® 4152 D SW 00413 HDPE High Density Polyethylene (HDPE), Injection Molded Lupolen®
LyondellBasell Lupolen® 4261 A HDPE, Blow Molding Grade High Density Polyethylene (HDPE), Blow Molding Grade Lupolen®
LyondellBasell Lupolen® 5021 D HDPE, Blow Molding Grade High Density Polyethylene (HDPE), Blow Molding Grade Lupolen®
LyondellBasell Lupolen® 5031 L HDPE, Injection Molding Grade High Density Polyethylene (HDPE), Injection Molded Lupolen®
LyondellBasell Lupolen® 5231 HX HDPE, Impact Grade High Density Polyethylene (HDPE), Impact Grade Lupolen®
LyondellBasell Lupolen® 5236 HX HDPE, Impact Grade High Density Polyethylene (HDPE), Impact Grade Lupolen®
LyondellBasell Lupolen® 5261 Z HDPE, Blow Molding Grade High Density Polyethylene (HDPE), Blow Molding Grade Lupolen®
LyondellBasell Lupolen® 5261 Z HI HDPE High Density Polyethylene (HDPE), Injection Molded Lupolen®
LyondellBasell Lupolen® 5261 ZS HDPE, Blow Molding Grade High Density Polyethylene (HDPE), Blow Molding Grade Lupolen®
LyondellBasell Lupolen® 5361 A HDPE, Blow Molding Grade High Density Polyethylene (HDPE), Blow Molding Grade Lupolen®
LyondellBasell Lupolen® 5621 D HDPE High Density Polyethylene (HDPE), Injection Molded Lupolen®
LyondellBasell Lupolen® 6021 D HDPE, Blow Molding Grade High Density Polyethylene (HDPE), Blow Molding Grade Lupolen®
LyondellBasell Lupolen® 6031 M HDPE, Injection Molding Grade High Density Polyethylene (HDPE), Injection Molded Lupolen®
LyondellBasell Lupolen® UHM 201 MDPE, Ultra-High Molecular Weight Medium Density Polyethylene (MDPE), Ultra High Molecular Weight Lupolen®
LyondellBasell Lupolen® UHM 301 MDPE, Ultra-High Molecular Weight Medium Density Polyethylene (MDPE), Ultra High Molecular Weight Lupolen®
LyondellBasell Lupolen® V 2520 J Ethylene Vinyl Acetate, Film Grade Ethylene Vinyl Acetate Copolymer (EVA), Film Grade Lupolen®
LyondellBasell Lupolen® V 2920 K Ethylene Vinyl Acetate, lnjection Molding Grade Ethylene Vinyl Acetate; Molded/Extruded Lupolen®
LyondellBasell Lupolen® V 3510 K Ethylene Vinyl Acetate, lnjection Molding Grade Ethylene Vinyl Acetate; Molded/Extruded Lupolen®
LyondellBasell Lupolen® V 3520 K Ethylene Vinyl Acetate Ethylene Vinyl Acetate; Molded/Extruded Lupolen®
LyondellBasell Lupolex FA LLDPE Linear Low Density Polyethylene (LLDPE), Film Grade Lupolex
LyondellBasell Montell 0300 Polybutene Polybutene Montell
LyondellBasell Montell 0800 Polybutene Polybutene Montell
LyondellBasell Montell 12C01G2 Clarity LLDPE Film Montell
LyondellBasell Montell 12C01G3 Clarity LLDPE Film Montell
LyondellBasell Montell 12C01G4 Clarity LLDPE Film Montell
LyondellBasell Montell 12C01G5 Clarity LLDPE Film Montell
LyondellBasell Montell 16501F3 Butene LLDPE Film Montell
LyondellBasell Montell 16501F4 Butene LLDPE Film Montell
LyondellBasell Montell 16501F6 Butene LLDPE Film Montell
LyondellBasell Montell 16501F7 Butene LLDPE Film Montell
LyondellBasell Montell 16501F8 Butene LLDPE Film Montell
LyondellBasell Montell 16502F3 Butene LLDPE Film Montell
LyondellBasell Montell 16502F7 Butene LLDPE Film Montell
LyondellBasell Montell 16502F8 Butene LLDPE Film Montell
LyondellBasell Montell 1900 UHMW Polyethylene HDPE Montell
LyondellBasell Montell 1900CM UHMW Polyethylene HDPE Montell
LyondellBasell Montell 1900H UHMW Polyethylene HDPE Montell
LyondellBasell Montell 1900LCM UHMW Polyethylene HDPE Montell
LyondellBasell Montell 8340 Polybutene-1 Polybutene Montell
LyondellBasell Montell 8640 Polybutene-1 Polybutene Montell
LyondellBasell Montell HB312CM UHMW Polyethylene HDPE Montell
LyondellBasell Montell HB320CM UHMW Polyethylene HDPE Montell
LyondellBasell Montell SE191 Polypropylene Impact Copolymer Polypropylene (PP) Montell
LyondellBasell Moplen EP/60 Bianco Polypropylene Copolymer Polypropylene Copolymer Moplen
LyondellBasell Moplen HP400H Polypropylene Homopolymer Polypropylene, Extrusion Grade Moplen
LyondellBasell Moplen HP400L Polypropylene Homopolymer Polypropylene, Molded Moplen
LyondellBasell Moplen HP400N Polypropylene Homopolymer Polypropylene, Molded Moplen
LyondellBasell Moplen HP550J Polypropylene Homopolymer Film Moplen
LyondellBasell Pro-fax 6301 Polypropylene Homopolymer, Flake Resin Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax 6323 Polypropylene Homopolymer, Easy Molding Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax 6329 Polypropylene Homopolymer, Improved Chemical Resistance Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax 6331 Polypropylene Homopolymer, Easy Molding Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax 6331NW Polypropylene Homopolymer, Nucleated/Antistat Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax 6331W Polypropylene Homopolymer, Antistat Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax 6523 Polypropylene Homopolymer, General Purpose Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax 6524 Polypropylene Homopolymer, Heat- and Extraction-Resistant Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax 7523 Polypropylene Impact Copolymer Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax 7531 Polypropylene Impact Copolymer Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax 7624 Polypropylene Impact Copolymer, Heat- and Extraction-Resistant Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax 7823 Polypropylene Impact Copolymer, Fractional Melt Flow Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax 8623 Polypropylene Impact Copolymer Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax PD702 Polypropylene Homopolymer, High Flow Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax PD702NW Polypropylene Homopolymer, Nucleated/Antistat Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax PF511 Polypropylene Homopolymer, Radiation Resistant Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax PF531 Polypropylene Homopolymer, Radiation Resistant Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax SA861 Polypropylene Random Copolymer, Cast Film Extrusion Film Pro-fax
LyondellBasell Pro-fax SB786 Polypropylene Impact Copolymer Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax SB787 Polypropylene Impact Copolymer Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax SB891 Polypropylene Impact Copolymer Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax SB912 Polypropylene Impact Copolymer Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax SD242 Polypropylene Impact Copolymer Polypropylene (PP) Pro-fax
LyondellBasell Pro-fax SG702 Polypropylene Impact Copolymer Polypropylene (PP) Pro-fax
LyondellBasell Pro-faxâ„¢ SG899 Polypropylene Copolymer Polypropylene Copolymer Pro-fax™