Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Pro-fax
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-fax 6524 Polypropylene Homopolymer, Heat- and Extraction-Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Features: heat and extraction-resistant polypropylene homopolymer resin, FDA acceptable, high resistance to solventsApplications: appliances, automotive under-the-hood applicationsMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: Pro-fax 6524 polypropylene homopolymer resin is highly resistant to aging at elevated temperatures in both wet and dry environments. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. It has a UL yellow card RTI, which applies to all colors. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785A
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.40 GPa
203 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.390 J/cm
0.731 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
UL RTI, Mechanical with Impact 115 °C
239 °F
Minimum thickness 0.040 inches.
Flammability, UL94 HB
HB
Minimum thickness 0.040 inches.