Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Pro-fax 6329 Polypropylene Homopolymer, Improved Chemical Resistance

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Pro-fax
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-fax 6329 Polypropylene Homopolymer, Improved Chemical Resistance.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Features: improved chemical resistance polypropylene homopolymer resin, FDA acceptable, easier processingApplications: closures, housewares, chairsMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: Pro-fax 6329 polypropylene homopolymer resin is designed for applications that require easier processing and improved chemical resistance properties. This resin is available in pelletized form. It meets FDA requirements in the Code of Federal Regulations in 21 FR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C
196 °F
ASTM D648