| Polyram BondyRam® 1001 Maleic Anhydride modified Homo-polypropylene coupling agent |
Additive/Filler for Polymer |
BondyRam®
|
| Polyram Bondyram® 1001CN Maleic Anhydride Modified Co-Polymer Propylene |
Polypropylene Copolymer |
BondyRam®
|
| Polyram Bondyram® 1004 Maleic Anhydride Modified Homo-Polypropylene |
Polypropylene (PP) |
BondyRam®
|
| Polyram Bondyram® 1010 Maleic Anhydride Modified Polypropylene |
Polypropylene (PP) |
BondyRam®
|
| Polyram Bondyram® 1101 Maleic Anhydride Modified Homo Propylene |
Polypropylene (PP) |
BondyRam®
|
| Polyram Bondyram® 4108 Maleic Anhydride Modified Linear Low Density Polyethylene |
Anhydride-Modified Polyethylene |
BondyRam®
|
| Polyram Bondyram® 5101 Maleic Anhydride Modified High Density Polyethylene |
Anhydride-Modified Polyethylene |
BondyRam®
|
| Polyram Bondyram® 5108 Maleic Anhydride Modified High Density Polyethylene |
Anhydride-Modified Polyethylene |
BondyRam®
|
| Polyram BondyRam® 6000 Maleic Anhydride grafted Acrylonitrile-Butadiene-Styrene coupling agent |
ABS Polymer |
BondyRam®
|
| Polyram BondyRam® 7001 Maleic Anhydride Modified Semi-crystalline EPDM Impact Modifier |
Additive/Filler for Polymer |
BondyRam®
|
| Polyram Bondyram® 7103 Maleic Anhydride Modified Ethylene-Alpha Olefin Copolymer |
Anhydride-Modified Polyethylene |
BondyRam®
|
| Polyram Bondyram® TL1207 Maleic Anhydride Modified Co-Polymer Polypropylene |
Polypropylene Copolymer |
BondyRam®
|
| Polyram Bondyram® TL1306 Maleic Anhydride Modified Polypropylene |
Polypropylene (PP) |
BondyRam®
|
| Polyram Bondyram® TL1308 Maleic Anhydride Modified Polypropylene |
Polypropylene (PP) |
BondyRam®
|
| Polyram Bondyram® TL4101A Maleic Anhydride Modified Polyethylene |
Anhydride-Modified Polyethylene |
BondyRam®
|
| Polyram Bondyram® TL4101B Maleic Anhydride Modified Linear Low Density Polyethylene |
LLDPE |
BondyRam®
|
| Polyram Bondyram® TL4109 Maleic Anhydride Modified Linear Low Density Polyethylene |
Anhydride-Modified Polyethylene |
BondyRam®
|
| Polyram Metal Cap PB360B60 Nylon 6, 60% Mineral Filled, Heavy Density |
Nylon 6 |
Metal Cap
|
| Polyram Metal Cap PL380Z81 Heavy Density Polyethylene, 81% Mineral Filled |
HDPE |
Metal Cap
|
| Polyram Metal Cap PPC370B60 Heavy Density Polypropylene, 60% Mineral Filled |
Polypropylene, Mineral Reinforced |
Metal Cap
|
| Polyram Metal Cap PPC371B73 Heavy Density Polypropylene, 73% Mineral Filled |
Polypropylene, Mineral Reinforced |
Metal Cap
|
| Polyram Metal Cap PPC372B73 Polypropylene, 73% Mineral Filled |
Polypropylene, Mineral Reinforced |
Metal Cap
|
| Polyram Metal Cap PPC373B72 Polypropylene, 72% mineral Filled |
Polypropylene, Mineral Reinforced |
Metal Cap
|
| Polyram PA310G8 Nylon 66, 40% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, 40% Glass Fiber Filled |
|
| Polyram PA500 Nylon 6.6, Flame Retardant |
Nylon 66, Unreinforced, Flame Retardant |
|
| Polyram PB302G50 Nylon 6, 50% Glass Fiber |
Nylon 6, 50% Glass Fiber Filled |
|
| Polyram PB330I8 Nylon 6, 40% Mineral/Glass Filled Heat Stabilized |
Nylon 6, 40% Mineral Filled |
|
| Polyram PF300G3 PBT, 15% Glass Fiber |
Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled |
|
| Polyram PlusTek PA103 Nylon 6.6, Injection Molding |
Nylon 66, Unreinforced |
PlusTek
|
| Polyram PlusTek PA106 Nylon 66 for Injection Molding, with Molybdenum Disulfide |
Nylon 66, MoS2 Filled |
PlusTek
|
| Polyram PlusTek PA108 Nylon6/6.6 Alloy for Injection Molding |
Nylon 66/6, Unreinforced |
PlusTek
|
| Polyram PlusTek PA112NT Nylon 6.6, PTFE Filled |
Nylon 66, PTFE Filled |
PlusTek
|
| Polyram PlusTek PA124 Nylon 6.6, Injection Molding |
Nylon 66, Unreinforced |
PlusTek
|
| Polyram PlusTek PA201 Nylon 66 for Extrusion |
Nylon 66, Extruded |
PlusTek
|
| Polyram PlusTek PA301G2 Nylon 6.6 for Injection Molding, 10% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, 10% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA301G3 Nylon 6.6, Heat Stabilized, 15% Glass Fiber |
Nylon 66, 20% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA301G4 Nylon 6.6, 20% Glass Fiber |
Nylon 66, 20% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA301G5 Nylon 6.6, Heat Stabilized, 25% Glass Fiber |
Nylon 66, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA301G50 Nylon 6.6, Heat Stabilized, 50% Glass Fiber |
Nylon 66, 50% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA301G6 Nylon 6.6, Heat Stabilized, 30% Glass Fiber |
Nylon 66, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA301G7 Nylon 6.6, Heat Stabilized 35% Glass Fiber |
Nylon 66, 40% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA303G33 Nylon 6.6, 33% Glass Fiber |
Nylon 66, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA303G4 Nylon 66 for Injection Molding, 20% Glass Fiber Reinforced, Heat Stabilized, Hydrolysis Resistant |
Nylon 66, 20% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA303G43 Nylon 6.6, 43% Glass Fiber |
Nylon 66, 40% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA303G5 Nylon 6.6, 25% Glass Fiber |
Nylon 66, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA303G50 Nylon 6.6, 50% Glass Fiber |
Nylon 66, 50% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA303G6 Nylon 6.6, Heat Stabilized, 30% Glass Fiber |
Nylon 66, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA303G6BK16 Nylon 6.6, 30% Glass Fiber reinforced, Heat Stabilized, Hydrolysis Resistant |
Nylon 66, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA305G6 Nylon 6.6, 30% Glass Fiber |
Nylon 66, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA309G6 Nylon 6.6, 30% Glass Fiber |
Nylon 66, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA313G43 Nylon 66 for Injection Molding, 43% Glass Fiber Reinforced, Heat Stabilized |
Nylon 66, 40% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA320G3 Nylon 6.6 for Injection Molding, 15% Glass Fiber Reinforced, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
PlusTek
|
| Polyram PlusTek PA320G4 Nylon 6.6, 20% Glass Fiber, Flame Retardant |
Nylon 66, 20% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA320G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
PlusTek
|
| Polyram PlusTek PA320G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
PlusTek
|
| Polyram PlusTek PA323G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
PlusTek
|
| Polyram PlusTek PA324G6 Nylon 6.6, UL-94 V-0 30% Glass Fiber |
Nylon 66, Glass Fiber Filled, Flame Retardant |
PlusTek
|
| Polyram PlusTek PA325G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
PlusTek
|
| Polyram PlusTek PA325G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant |
Nylon 66, Glass Fiber Filled, Flame Retardant |
PlusTek
|
| Polyram PlusTek PA340S05 Nylon 6.6 for Injection Molding, 5% Glass-beads Reinforced, Heat Stabilized |
Nylon 66, Glass Bead Filled |
PlusTek
|
| Polyram PlusTek PA340S4 Nylon 66 for Injection Molding, 20% Glass-Beads Reinforced |
Nylon 66, Glass Bead Filled |
PlusTek
|
| Polyram PlusTek PA340S6 Nylon 6.6, 30% Glass beads |
Nylon 66, Glass Bead Filled |
PlusTek
|
| Polyram PlusTek PA340S8 Nylon 6.6 for Injection Molding, 40% Glass-beads Reinforced |
Nylon 66, Glass Bead Filled |
PlusTek
|
| Polyram PlusTek PA341G9 Nylon 6.6, 45% Glass Fiber |
Nylon 66, 50% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA350M4 Nylon 6.6 for Injection Molding, 20% Mineral Reinforced |
Nylon 66, 20% Mineral Filled |
PlusTek
|
| Polyram PlusTek PA351M8 Nylon 6.6 for Injection Molding, 40% Mineral Reinforced |
Nylon 66, 40% Mineral Filled |
PlusTek
|
| Polyram PlusTek PA352M6 Nylon 6.6, 30% Low Friction Mineral Filled |
Nylon 66, 30% Mineral Filled |
PlusTek
|
| Polyram PlusTek PA355M6 Nylon 6.6 for Injection Molding, 30% Mineral Filled, Flame Retardant |
Nylon 66, 30% Mineral Filled |
PlusTek
|
| Polyram PlusTek PA360G6 Nylon 6.6, 30% Glass Fiber |
Nylon 66, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA4501G6 Nylon 66, 30% Glass Fiber Reinforced, Low Friction |
Nylon 66, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA4801G6 Nylon 6.6, 30% Glass Fiber Reinforced, PTFE lubricated |
Nylon 66, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA517 Nylon 6.6, Flame Retardant |
Nylon 66, Unreinforced, Flame Retardant |
PlusTek
|
| Polyram PlusTek PA600 Nylon 6.6, Heat Stabilized |
Nylon 66, Heat Stabilized |
PlusTek
|
| Polyram PlusTek PA602 Nylon 6.6, Heat Stabilized |
Nylon 66, Heat Stabilized |
PlusTek
|
| Polyram PlusTek PA604 Nylon 6.6, Heat Stabilized |
Nylon 66, Heat Stabilized |
PlusTek
|
| Polyram PlusTek PA7001G7BK11 Nylon 66, 35% Glass Fiber Reinforced, Heat and UV Stabilized, Hydrolysis Resistant |
Nylon 66, 40% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA700BL10 Nylon 6.6 for Injection Molding, UV Stabilized |
Nylon 66, Unreinforced |
PlusTek
|
| Polyram PlusTek PA7800G33 Nylon 6.6 for Injection Molding, 33% Glass Fiber Reinforced, Heat Stabilized, Impact Modified |
Nylon 66, Glass Reinforced, Impact Grade |
PlusTek
|
| Polyram PlusTek PA801 Nylon 6.6 Copolymer for Injection Molding, Impact Modified |
Nylon 66, Impact Grade |
PlusTek
|
| Polyram PlusTek PA803 Nylon 6.6 for Injection Molding, Impact Modified |
Nylon 66, Impact Grade |
PlusTek
|
| Polyram PlusTek PA804 Nylon 6.6 for Injection Molding, Impact Modified |
Nylon 66, Impact Grade |
PlusTek
|
| Polyram PlusTek PA810 Nylon 6.6, Impact Modified |
Nylon 66, Impact Grade |
PlusTek
|
| Polyram PlusTek PA823M6 Nylon 6.6 for Injection Molding, 30% Minerals Reinforced, Impact Modified |
Nylon 66, Mineral Filled, Impact Grade |
PlusTek
|
| Polyram PlusTek PA830 Nylon 6.6, Impact Modified |
Nylon 66, Impact Grade |
PlusTek
|
| Polyram PlusTek PA840G13 Nylon 66 for Injection Molding, 13% Glass Fiber Reinforced, Impact Modified, Heat Resistant |
Nylon 66, Glass Reinforced, Impact Grade |
PlusTek
|
| Polyram PlusTek PA840G3 Nylon 6.6, 15% Glass Fiber |
Nylon 66, 20% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA840G7 Nylon 6.6 for Injection Molding, 35% Glass Fibers Reinforced, Impact Modified |
Nylon 66, Glass Reinforced, Impact Grade |
PlusTek
|
| Polyram PlusTek PA841 Nylon 6.6, Impact Modified |
Nylon 66, Impact Grade |
PlusTek
|
| Polyram PlusTek PA860 Nylon 6.6, Impact Modified |
Nylon 66, Impact Grade |
PlusTek
|
| Polyram PlusTek PA862 Nylon 6.6 for Injection Molding, High Impact Modified |
Nylon 66, Impact Grade |
PlusTek
|
| Polyram PlusTek PA865G6 Nylon 6.6, 30% Glass Fiber |
Nylon 66, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA870G33 Nylon 6.6, 33% Glass Fiber |
Nylon 66, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PA880 Nylon 6.6, Impact Modified |
Nylon 66, Impact Grade |
PlusTek
|
| Polyram PlusTek PB140 Nylon 6, Injection Molding |
Nylon 6, Unreinforced |
PlusTek
|
| Polyram PlusTek PB142 Nylon 6 for Injection Molding |
Nylon 6, Unreinforced |
PlusTek
|
| Polyram PlusTek PB150 Nylon 6, Injection Molding |
Nylon 6, Unreinforced |
PlusTek
|
| Polyram PlusTek PB300G3 Nylon 6, 15% Glass Fiber |
Nylon 6, 20% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PB300G33 Nylon 6, 33% Glass Fiber |
Nylon 6, 30% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PB300G5 Nylon 6, 15% Glass Fiber |
Nylon 6, 20% Glass Fiber Filled |
PlusTek
|
| Polyram PlusTek PB300G6 Nylon 6, 30% Glass Fiber |
Nylon 6, 30% Glass Fiber Filled |
PlusTek
|