Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 3615 General Purpose Glass Cloth Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 3615 General Purpose Glass Cloth Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Glass Cloth Tape 3615 is a general purpose, easy unwind tape coated with a silicone adhesive for many applications requiring high-temperature resistance, high adhesion, and a very strong, abrasion-resistant backing.Information provided by 3M
Physical Properties Metric English Comments
Thickness 127 microns
5.00 mil
Backing; ASTM D3752
178 microns
7.00 mil
Total; ASTM D3752
Mechanical Properties Metric English Comments
Tensile Strength at Break 174.4 MPa
25290 psi
ASTM D3759
Elongation at Break 7.0 %
7.0 %
ASTM D3759
Peel Strength 0.38347 kN/m
2.1875 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
288 °C
550 °F
Intermittent
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Descriptive Properties Value Comments
Adhesive Type Silicone
Appearance White