| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 127 microns | 5.00 mil | Nominal |
|
DuPont™ Nomex® E56 Paper, 5 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
|
|||
| Thickness | 127 microns | 5.00 mil | Backing; ASTM D3752 |
|
3M 399FR Flame Retardant Glass Cloth Tape
3M™ Flame Retardant Glass Cloth Tape 399FR has an acrylic adhesive for many applications requiring high adhesion, an abrasion-resistant backing and flame retardant properties. This product is typic..
|
|||
| Thickness | 127 microns | 5.00 mil | Substrate |
|
Arlon 30400R040 0.04" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should..
|
|||
| Thickness | 127 microns | 5.00 mil | Kodacel Carrier |
|
Arlon 30570XA015 0.015" (0.381mm) Uncured/Unsupported Silicone Rubber on a Release Carrier
Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Gray silicone gum on polymer linerThis data represents typical values for the production material. Th..
|
|||
| Thickness | 127 microns | 5.00 mil | PET Carrier; Arlon SQA-TMS-003 |
|
Arlon 32580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a PET Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data s..
|
|||
| Thickness | 127 microns | 5.00 mil | Carrier; Arlon SQA-TMS-003 |
|
Arlon 41300R062 0.062" Uncured Silicone Rubber on Holland Cloth
Design/Construction:Interleave: 3.0 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Holland ClothThis data represents typical values for the production material and should not be used as m..
|
|||
| Thickness | >= 127 microns | >= 5.00 mil | Side 2 |
|
Arlon 49576R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat..
|
|||
| Thickness | 127 microns | 5.00 mil | Side 1, Cured Rubber Layer |
|
Arlon 55579R043 0.043" (1.09 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured layer on top of a cured layer on one side Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production materi..
|
|||
| Thickness | 127 - 152 microns | 5.00 - 6.00 mil | with adhesive |
|
3M Scotchcal™ IJ8171 Perforated Window Graphic Film
Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black..
|
|||
| Thickness | 127 microns | 5.00 mil | Tape |
|
3M XT2112-AGT Hi-Tack Adhesive Transfer Tape
3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range o..
|
|||
| Thickness | 127 microns | 5.00 mil | Substrate |
|
Arlon 41580R030 0.030" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
|
|||
| Thickness | 127 microns | 5.00 mil | Substrate |
|
Arlon 41600R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
|
|||
| Thickness | 127 microns | 5.00 mil | Prime Coated 1165 Fiberglass, Substrate |
|
Arlon 44576B009A 0.0085" (0.216 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of..
|
|||
| Thickness | 127 - 152 microns | 5.00 - 6.00 mil | Side 1 |
|
Arlon 51571S020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
|
|||
| Thickness | 127 microns | 5.00 mil | Side 2; Arlon SQA-TMS-003 |
|
Arlon 54331R014 0.014" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: Blue LDPESide 1: Uncured Silicone RubberSubstrate: Style 2116 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Blue LDPEThis data represents typical valu..
|
|||
| Thickness | 127 microns | 5.00 mil | side 1; Arlon SQA-TMS-003 |
|
Arlon 55141R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE
|
|||
| Thickness | 127 microns | 5.00 mil | Adhesive |
|
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
|
|||
| Thickness | 127 microns | 5.00 mil | Tape Only |
|
3M F-9465PC Adhesive Transfer Tape
3M™ Adhesive Transfer Tape F-9465PC is a 5 mil thick adhesive transfer tape which has been formulated for bonding to many flexible vinyls and to resist the effects of plasticizer migration in flexi..
|
|||
| Thickness | 127 microns | 5.00 mil | Backing; ASTM D3752 |
|
3M 5181 General Purpose PTFE Skived Film Tapes
3M™ General Purpose PTFE Skived Film Tapes are film backing with a silicone adhesive.Information provided by 3M
|
|||
| Thickness | 127 microns | 5.00 mil | Total |
|
Parker Chomerics CHO-FOIL CAD Shielding Tape
Conductive Adhesive Aluminum FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ..
|
|||
| Thickness | 127 microns | 5.00 mil | Facestock |
|
3M OFL020N Outdoor UL Recognized Lexan Label Products
3M™ Outdoor UL Recognized Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P..
|
|||
| Thickness | 127 microns | 5.00 mil | ASTM D3652 |
|
3M Scotchgard™ 1001 Protective Film
3M™ Scotchgard™ Protective 1001 is an optically transparent, pressure-sensitive polyester film tape designed to protect surfaces from intentional and unintentional mutilation, scratching, etching ..
|
|||
| Thickness | 127 microns | 5.00 mil | Substrate |
|
Arlon 41580R020 0.020" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
|
|||
| Thickness | 127 microns | 5.00 mil | Substrate |
|
Arlon 41580R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
|
|||
| Thickness | 127 microns | 5.00 mil | Prime Coated 1165 Fiberglass, Substrate |
|
Arlon 44570R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Layers Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be use..
|
|||
| Thickness | 127 microns | 5.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 44570XB025 0.025" Uncured Silicone Rubber with Fiberglass
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not b..
|
|||
| Thickness | 127 microns | 5.00 mil | Prime Coated 1165 Fiberglass, Substrate |
|
Arlon 44602W020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberProduct Use: Flexible heater insulationAppearance: White silicone rubber on fiberglassThis data represents typical values for the production material..
|
|||
| Thickness | 127 microns | 5.00 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 44278R018 0.018" Uncured/Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate
Design/Construction:Interleave 1: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEUL..
|
|||
| Thickness | >= 127 microns | >= 5.00 mil | Side 1 |
|
Arlon 44570R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Layers Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be use..
|
|||
| Thickness | 127 microns | 5.00 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 48B10R005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassThis data represents typical values for the production material. The data should not be us..
|
|||