3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmness and strength on a variety of surfaces including high surface energy (HSE) and low surface energy (LSE) plastics, as well as, metals.Information provided by 3M
Physical Properties Metric English Comments
Thickness 22.9 microns
0.900 mil
Adhesive
38.1 microns
1.50 mil
Liner
102 microns
4.00 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.153 kN/m
0.875 pli
LD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.153 kN/m
0.875 pli
LD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.20817 kN/m
1.1875 pli
LD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
0.23008 kN/m
1.3125 pli
Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
0.2849 kN/m
1.625 pli
HD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.3287 kN/m
1.875 pli
HD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330
0.66833 kN/m
3.8125 pli
LD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.701 kN/m
4.00 pli
LD Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
0.7669 kN/m
4.375 pli
LD Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.7669 kN/m
4.375 pli
HD Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
0.77789 kN/m
4.4375 pli
Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330
0.79981 kN/m
4.5625 pli
HD Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.79981 kN/m
4.5625 pli
HD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.88746 kN/m
5.0625 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
50.0 °C
122 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 320 Acrylic