| Category | Polymer , Adhesive |
| Manufacturer | 3M |
| Trade Name | Bumpon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | 3M Bumpon™ SJ5904 Resilient Rollstock.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.640 g/cc | 0.0231 lb/in³ | |
| Thickness | 6350 microns | 250 mil |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore M | 36 | 36 | Polyurethane, medium foam |
| Tensile Strength at Break | 0.830 MPa | 120 psi | Die A; ASTM D412 |
| Elongation at Break | 100 % | 100 % | Die A; ASTM D412 |
| Coefficient of Friction | >= 1.0 | >= 1.0 | Stainless Steel, Kinetic |
| >= 1.0 | >= 1.0 | Glass, Kinetic | |
| 0.80 - 1.4 | 0.80 - 1.4 | Formica laminate, Kinetic | |
| 0.80 - 1.4 | 0.80 - 1.4 | Wood, Kinetic | |
| Peel Strength | 0.526 kN/m | 3.00 pli | 90°, Adhesion to Polypropylene |
| 1.93 kN/m | 11.0 pli | 90°, Adhesion to Polystyrene | |
| 4.38 kN/m | 25.0 pli | 90°, Adhesion to ABS | |
| 4.38 kN/m | 25.0 pli | 90°, Adhesion to Stainless Steel | |
| 4.38 kN/m | 25.0 pli | 90°, Adhesion to Aluminum | |
| Taber Abrasion, mg/1000 Cycles | 1.8 - 2.0 | 1.8 - 2.0 | H18, 1 kg; ASTM C501 |
| Compression Set | 12 % | 12 % | ASTM D1056 |
| 14 % | 14 % | 50% deflection; ASTM D1056 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
| 66.0 °C | 151 °F | Service | |
| 107 °C | 225 °F | Intermittent Exposure | |
| Minimum Service Temperature, Air | -34.0 °C | -29.2 °F | Service |
| 5.00 °C | 41.0 °F | Application | |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 5.51 kV/mm | 140 kV/in | ASTM D1000 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Adhesive Type | A-20 (acrylic) | |
| Appearance | Black |