Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchcast™ 5388 Electrical Epoxy Powder Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer 3M
Trade Name Scotchcast™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcast™ 5388 Electrical Epoxy Powder Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M Scotchcast Electrical Resin 5388 is a one-part, blue pigmented, rapid heat curing powder resin, designed to provide a continuous, tough moisture and chemical resistant dielectric coating to a variety of substrates. Resin 5388 is manufactured by a fusion blend process, insuring that each individual particle of powder contains all the components necessary to effect a complete cure and attain stated performance properties. Resin 5388 is applied to a cold object via the electrostatic fluid bed process. The negatively charge resin particles are attracted to the grounded object to be coated. Coating thicknesses up to 25 mils may be obtained. Because of its superior charging capabilities resin 5388 exhibits excellent slot penetration on motor stators and armatures. Uses for electrical resin 5388 include moisture-proofing and insulating armatures, stators, buss mars and toroid cores.Information provided by 3M
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
cured; ASTM D794
Mechanical Properties Metric English Comments
Impact Test 11.3 J
8.33 ft-lb
12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester
Electrical Properties Metric English Comments
Dielectric Strength 43.3 kV/mm
1100 kV/in
12 to 15 mil coating; ASTM D149
Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 232 °C
0.0500 hour

@Temperature 450 °F
6.00 min

@Temperature 204 °C
0.100 hour

@Temperature 399 °F
15.0 min

@Temperature 177 °C
0.250 hour

@Temperature 351 °F
Gel Time 0.250 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 193 °C
0.250 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 379 °F
hot plate
Shelf Life 18.0 Month

@Temperature <=16.0 °C
18.0 Month

@Temperature <=60.8 °F
Descriptive Properties Value Comments
Appearance Blue
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved