Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ACC EP RSP EPI Engineered Polymers Silicone Polyurea

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC EP RSP EPI Engineered Polymers Silicone Polyurea.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
EP RSP Silicone Polyurea, “Powered by Reactamine®Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RSP displays extremely fast cure times with excellent adhesions to different substrates. EP RSP can be spray applied at temperatures ranging from 20°F to 150°F. EP RSP has excellent chemical and water resistance. EP RSP has a temperature range of -40°F to 350°F. EP RSP conforms to USDA and FDA guidelines for incidental food contact. Applications: EP RSP adheres well to several substrates including concrete, steel, and wood. Some typical uses include: SECONDARY CONTAINMENT WASTEWATER LAGOON AND POOL LININGS ANTI GRAFFITI COLD STORAGE AREAS WASH BAY AND SHOWER LININGS COOLING TOWERS PETROCHEMICAL REFINERIES OILFIELD PIPELINE COATINGS WATER PROOFING SEWER LINERS MANHOLE RESTORATION INDUSTRIAL FLOORING BRIDGE COATINGSPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Viscosity 600 cP
600 cP
B Side
800 cP
800 cP
A Side
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength, Yield 15.5 MPa
2250 psi
ASTM D412
Elongation at Break 750 %
750 %
ASTM D412
100% Modulus 0.00896 GPa
1.30 ksi
ASTM D412
300% Modulus 0.0103 GPa
1.49 ksi
ASTM D412
Adhesive Bond Strength >= 1.72 MPa
>= 250 psi
Wood (no primer), Delamination; ASTM D4541 Elcometer
2.07 MPa
300 psi
Concrete (epoxy), Concrete Failure; ASTM D4541 Elcometer
2.76 MPa
400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
>= 6.21 MPa
>= 900 psi
Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer
>= 10.3 MPa
>= 1500 psi
Steel (no primer), Substrate Failure; ASTM D4541 Elcometer
Tear Strength 71.9 kN/m
410 pli
ASTM D412
Taber Abrasion, mg/1000 Cycles 22
22
CS17 WHEEL, 1kg per 1000 cycles; ASTM D4060
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F
ASTM Pensky-Martin
Processing Properties Metric English Comments
Cure Time 0.267 - 0.583 min
0.00444 - 0.00972 hour
Tack Free Time
Gel Time 0.150 min
0.150 min
Fast
0.3667 min
0.3667 min
Slow
Descriptive Properties Value Comments
Color Most primary colors, including white.
Flexibility Pass
ASTM D1737, 1/8"Mandrel
Resistance to 1,1,1-Trichlorethane Conditional
Resistance to Acetic Acid (100%) Recommended Conditional
Resistance to Acetone Recommended Conditional
Resistance to Ammonium Hydroxide (50%) Recommended
Resistance to Benzene Recommended Conditional
Resistance to Brine-Saturated H2O Recommended
Resistance to Brine-Saturated H<sub>2</sub>O (310g/l)
Resistance to Chlorinated H2O Recommended
Resistance to Clorox® (10%) H2O Recommended
Resistance to Diesel Fuel Recommended Conditional
Resistance to Gasoline Recommended Conditional
Resistance to Gasoline/ 5% Methanol Recommended Conditional
Resistance to Gasoline/5% MTBE Recommended Conditional
Resistance to H2O Recommended
Resistance to H2O (14 days at 82°C) Recommended
Resistance to Hydraulic Fluid (oil) Recommended Conditional
Resistance to Hydrochloric Acid (20%) Recommended
Resistance to Hydrofluoric Acid(50%) Recommended
Resistance to Isopropyl Alcohol Recommended
Resistance to Lactic Acid Recommended Conditional
Resistance to MEK Recommended Conditional
Resistance to Methanol Recommended
Resistance to Methylene chloride Conditional
Resistance to Mineral Spirits Recommended Conditional
Resistance to Motor Oil Recommended
Resistance to MTEB Conditional
Resistance to Muriatic Acid (10%) Recommended
Resistance to NaCl/H2O (10%) Recommended
Resistance to Nitric Acid ( Recommended
Resistance to Phosphoric Acid (10%) Recommended
Resistance to Phosphoric Acid (50%) Not Recommended
Resistance to Potassium Hydroxide (10%) Recommended
Resistance to Potassium Hydroxide (20%) Recommended, Discoloration
Resistance to Propylene Carbonate Recommended Conditional
Resistance to Skydrol® Conditional
Resistance to Sodium Bicarbonate Recommended
Resistance to Sodium Hydroxide (25%) Recommended
Resistance to Sodium Hydroxide (50%) Recommended
Resistance to Sodium Hypochlorite (10%) Recommended
Resistance to Stearic Acid Recommended
Resistance to Sugar/H2O Recommended
Resistance to Sulfuric Acid (>50%) Recommended Conditional
Resistance to Sulfuric Acid (10%) Recommended
Resistance to Toluene Recommended
Resistance to Trisodium Phosphate Recommended
Resistance to Vinegar/ H2O (5%) Recommended
Resistance to Xylene Recommended Conditional