AKG Polymers Vision PP PPH Jazz0502dark Polypropylene Homopolymer Compound

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer AKG Polymers
Trade Name Vision PP
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF AKG Polymers Vision PP PPH Jazz0502dark Polypropylene Homopolymer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineering, Construction, Horticulture, ElectronicsInformation provided by AKG Polymers BV
Physical Properties Metric English Comments
Density 0.900 - 0.920 g/cc
0.0325 - 0.0332 lb/in³
Internal
Filler Content <= 5.0 %
<= 5.0 %
Internal
Melt Flow 3.0 - 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 - 7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 68 - 72
68 - 72
Internal
Flexural Modulus >= 1.25 GPa
>= 181 ksi
ISO 178
Charpy Impact, Notched >= 0.350 J/cm²

@Temperature 23.0 °C
>= 1.67 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Falling Dart Impact >= 1.99 J

@Temperature 23.0 °C
>= 1.47 ft-lb

@Temperature 73.4 °F
Internal
Descriptive Properties Value Comments
Application Area horticulture
Color Dark jazz
Non-virgin Polymer Content (%), Min 95
Process thermo forming