ATI Allegheny Ludlum Grade 2 Titanium (UNS R50400)

Category Metal , Nonferrous Metal , Titanium Alloy , Unalloyed/Modified Titanium
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum Grade 2 Titanium (UNS R50400).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Uses: CPI equipment, industrial components, condenser tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum.
Physical Properties Metric English Comments
Density 4.52 g/cc
0.163 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 160
160
Tensile Strength, Ultimate 483 MPa
70100 psi
Tensile Strength, Yield 345 MPa

@Strain 0.200 %
50000 psi

@Strain 0.200 %
Elongation at Break 27 %
27 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe <= 0.30 %
<= 0.30 %
Nitrogen, N <= 0.030 %
<= 0.030 %
Oxygen, O <= 0.25 %
<= 0.25 %
Titanium, Ti >= 99.3 %
>= 99.3 %
as balance