Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ATI Allvac® REX 734™ UNS S31675 Specialty Steel

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer ATI Allvac
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® REX 734™ UNS S31675 Specialty Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Uses: Medical and surgical devices; forged mono-block hip stems.Property values are for samples in the metallurgical condition: As rolled, warm worked.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 7.89 g/cc
0.285 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 22
22
Tensile Strength, Ultimate 860 MPa
125000 psi
Tensile Strength, Yield 485 MPa

@Strain 0.200 %
70300 psi

@Strain 0.200 %
Elongation at Break 45 %
45 %
Reduction of Area 70 %
70 %
Component Elements Properties Metric English Comments
Carbon, C 0.040 %
0.040 %
Chromium, Cr 20.8 %
20.8 %
Copper, Cu 0.12 %
0.12 %
Iron, Fe 62 %
62 %
as balance
Manganese, Mn 3.12 %
3.12 %
Molybdenum, Mo 2.5 %
2.5 %
Nickel, Ni 10 %
10 %
Niobium, Nb (Columbium, Cb) 0.52 %
0.52 %
Nitrogen, N 0.38 %
0.38 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.38 %
0.38 %
Sulfur, S 0.0050 %
0.0050 %