Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROPRENE® ATPR ECATPR2040 Black Thermoplastic SEBS Rubber

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE® ATPR
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® ATPR ECATPR2040 Black Thermoplastic SEBS Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AAROPRENE® ATPR 2000 Series Elastomeric CompoundFeatures: A black, thermoplastic SEBS Rubber compound specifically designed for the injection molding of industrial gaskets.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Melt Flow 15 g/10 min
15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
ASTM D2240
Tensile Strength at Break 6.21 MPa
900 psi
ASTM D412
Elongation at Break 800 %
800 %
ASTM D412
Modulus of Elasticity 2.76 GPa
400 ksi
ASTM D412
Tensile Modulus 0.00124 GPa
0.180 ksi
ASTM D412
Taber Abrasion, mg/1000 Cycles 290
290
ASTM D1044
Processing Properties Metric English Comments
Feed Temperature 79.4 °C
175 °F
Nozzle Temperature 235 °C
455 °F
Injection Pressure 3.45 - 4.83 MPa
500 - 700 psi
Back Pressure 0.345 MPa
50.0 psi
Cycle Time - Injection 1.0 sec
1.0 sec
Screw Speed 40 rpm
40 rpm