Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast/AboCure 8109-10

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Abatron
Trade Name AboCast/AboCure
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast/AboCure 8109-10.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Processing: 100% solids; 100/130 ratio; Potlife: 6-8 days/20°C (68°F); 1-2 days 40°C (105°F), 10-15 hours at 60°C (140°F); cures im: 8 h/80°C (175°F), 6 h/100°C (212°F), 4 h/120°C (250°F); mix thoroughly at RT, heat to desired viscosity, apply to clean, dry surface.Applications: Impregnating and potting.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Water Absorption 0.20 - 0.35 %
0.20 - 0.35 %
(60x10X4 mm bar) after 10 days at 20°C (77°F)
0.30 - 0.45 %
0.30 - 0.45 %
(60x10X4 mm bar) after 1 hour at 100°C (212°F)
Viscosity 3500 - 6500 cP
3500 - 6500 cP
30 - 60 cP

@Temperature 60.0 °C
30 - 60 cP

@Temperature 140 °F
350 - 650 cP

@Temperature 40.0 °C
350 - 650 cP

@Temperature 104 °F
Vapor Pressure 0.00133 bar

@Temperature 180 °C
1.00 torr

@Temperature 356 °F
AboCast
0.00133 bar

@Temperature 100 °C
1.00 torr

@Temperature 212 °F
AboCure
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.15 MPa
7999 psi
Modulus of Elasticity 2.068 GPa
299.9 ksi
Flexural Yield Strength 86.18 MPa
12500 psi
Compressive Yield Strength 89.63 MPa
13000 psi
Thermal Properties Metric English Comments
CTE, linear 95.0 - 105 µm/m-°C

@Temperature 20.0 °C
52.8 - 58.3 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 70.0 °C
158 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.50e+16 ohm-cm
>= 1.50e+16 ohm-cm
Dielectric Constant 2.5 - 3.0

@Frequency 1000 Hz
2.5 - 3.0

@Frequency 1000 Hz
2.6 - 3.1

@Frequency 1e+6 Hz
2.6 - 3.1

@Frequency 1e+6 Hz
2.7 - 3.2

@Frequency 50 Hz
2.7 - 3.2

@Frequency 50 Hz
Dielectric Strength 11.8 - 15.7 kV/mm

@Thickness 3.17 mm
300 - 400 kV/in

@Thickness 0.125 in
Short time value
Dissipation Factor 0.0030 - 0.0060

@Frequency 50 Hz
0.0030 - 0.0060

@Frequency 50 Hz
0.0050 - 0.0070

@Frequency 1000 Hz
0.0050 - 0.0070

@Frequency 1000 Hz
0.010 - 0.015

@Frequency 1e+6 Hz
0.010 - 0.015

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Pot Life 600 - 900 min

@Temperature 60.0 °C
600 - 900 min

@Temperature 140 °F
1440 - 2880 min

@Temperature 40.0 °C
1440 - 2880 min

@Temperature 104 °F
8640 - 11520 min

@Temperature 20.0 °C
8640 - 11520 min

@Temperature 68.0 °F