Polymer Property : Dielectric Strength = 11.8 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Dielectric Strength 11.8 kV/mm
300 kV/in
ASTM D149
DSM Biomedical PurSil® AL 5 Aliphatic Thermoplastic Silicone Polyether Urethane  (discontinued **)
PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether..
Dielectric Strength 11.8 - 45.0 kV/mm
300 - 1140 kV/in
Average value: 19.3 kV/mm Grade Count:15
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Dielectric Strength 11.8 kV/mm
300 kV/in
ASTM D149
Plenco 202 Black General Purpose Woodflour Filled Phenolic Molding Compound  (discontinued **)
Plaslok 202 is a two-stage, woodflour-filled phenolic molding compound formulated to provide improved impact and fatigue strength, good dimensional stability and excellent molded finish for automoti..
Dielectric Strength 11.8 - 90.0 kV/mm
300 - 2290 kV/in
Average value: 24.1 kV/mm Grade Count:46
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Dielectric Strength 11.8 kV/mm
300 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® HDPE GF10 CC 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc.
Dielectric Strength 11.8 kV/mm
300 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PEEK 450 BK
Availability: North AmericaForms: PelletsFeatures: High ViscosityAppearance: BlackInformation provided by TP Composites, Inc.
Dielectric Strength 11.8 kV/mm
300 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PP 0123 C Polypropylene
Availability: North AmericaForms: PelletsFeatures: Copolymer and Thermally ConductiveInformation provided by TP Composites, Inc.
Dielectric Strength 11.8 kV/mm
300 kV/in
Step by step; ASTM D149
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade
Durez 29502 B brown phenolic is a two stage, glass and mineral filled, special purpose molding material with improved mechanical and heat resistant properties. It is formulated for close tolerance ..
Dielectric Strength 11.8 kV/mm
300 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Luriblend® HDPE TL10
Availability: North AmericaForms: PelletsAdditive: PTFE LubricantInformation provided by TP Composites, Inc.
Dielectric Strength 11.8 kV/mm
300 kV/in
Short Time; ASTM D149
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Injection Grade
Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s..
Dielectric Strength 11.8 kV/mm
300 kV/in
Short Time; ASTM D149
Plenco 08112 Polyester BMC, Compression Molded
PLENCO 08112 is a renumber of PlasGlas 10112. PLENCO 08112 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co..
Dielectric Strength 11.8 - 18.7 kV/mm
300 - 475 kV/in
ASTM D149
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp
Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
Dielectric Strength 11.8 - 18.7 kV/mm
300 - 475 kV/in
ASTM D149
Eastman Tenite 285E3720005 Butyrate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Dielectric Strength 11.8 - 18.7 kV/mm
300 - 475 kV/in
ASTM D149
Eastman Tenite 307A4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Dielectric Strength 11.8 - 18.7 kV/mm
300 - 475 kV/in
ASTM D149
Eastman Tenite 350A0096914 Propionate Natural
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Dielectric Strength 11.8 - 18.7 kV/mm
300 - 475 kV/in
ASTM D149
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp
Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss..
Dielectric Strength 11.8 - 18.7 kV/mm
300 - 475 kV/in
ASTM D149
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Dielectric Strength 11.8 - 18.7 kV/mm
300 - 475 kV/in
ASTM D149
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Dielectric Strength 11.8 - 18.7 kV/mm
300 - 475 kV/in
ASTM D149
Eastman Tenite 485E3720023 Butyrate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Dielectric Strength 11.8 kV/mm
300 kV/in
ASTM D149
Arlon 30300R062 0.062" (1.57 mm) Uncured Silicone Rubber on Kodacel Carrier
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberCarrier: KodacelAppearance: Red silicone gum on polymer linersThis data represents typical values for the production mate..
Dielectric Strength 11.8 kV/mm

@Thickness 1.91 mm
300 kV/in

@Thickness 0.0750 in
Environmental Sealing Compound; ASTM D149
3M 7660-S-HSG Cold Shrink QT-III Silicone Rubber Skirted Termination Kits
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7650-S-HSG and 7660-S-HSG Series, are designed for applications requiring a high-ampacity ground. Each kit contains one-piece, skirt..
Dielectric Strength 11.8 kV/mm
300 kV/in
Aremco Ceramacast™ 675-N High Temperature Potting & Casting Material Aluminum Nitride
Fine grain aluminum nitride castable with high thermal conductivity.
Dielectric Strength 11.8 kV/mm
300 kV/in
Short Time
Bulk Molding Compounds BMC 1902 Mineral Filled Alkyd
BMC 1902 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression molding. It was developed primarily for applications requiring very good impact and flex..
Dielectric Strength 11.8 kV/mm
300 kV/in
Short Time
Bulk Molding Compounds BMC 501E Mineral Filled, Glass Reinforced Polyester
BMC 501E molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a product with good overall electrical properties, flame..
Dielectric Strength 11.8 - 45.0 kV/mm
300 - 1140 kV/in
Average value: 25.8 kV/mm Grade Count:12
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..
Dielectric Strength 11.8 - 18.7 kV/mm
300 - 475 kV/in
ASTM D149
Eastman Tenite 360A4861301 Propionate Clear, Trsp  (discontinued **)
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Dielectric Strength 11.8 kV/mm
300 kV/in
Short Time; 1/8 inch; ASTM D149
G-5 Fiberglass Melamine Laminate Sheet
This material is very hard, flame resistant, and has excellent electrical properties. G-5 has high arc and heat resistance. It used for switch board panels, arc barriers, circuit breaker parts, and ..
Dielectric Strength 11.8 - 100 kV/mm
300 - 2540 kV/in
Average value: 26.8 kV/mm Grade Count:105
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..