| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded |
| Manufacturer | Aclo Compounders |
| Trade Name | Accucomp |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Accucomp ABS ABS809SL Extrusion Grade.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | MD; ASTM D955 |
| Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 92 | 92 | ASTM D785 |
| Tensile Strength at Break | 30.0 MPa | 4350 psi | ASTM D638 |
| Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
| Elongation at Break | 25 % | 25 % | ASTM D638 |
| Elongation at Yield | 4.0 % | 4.0 % | ASTM D638 |
| Tensile Modulus | 1.498 GPa | 217.3 ksi | ASTM D638 |
| Flexural Strength | 54.0 MPa | 7830 psi | ASTM D790 |
| Flexural Modulus | 2.099 GPa | 304.5 ksi | ASTM D790 |
| Izod Impact, Notched | 5.23 J/cm | 9.80 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 86.1 °C | 187 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 73.9 °C | 165 °F | |
| Flammability, UL94 | HB @Thickness 1.59 mm |
HB @Thickness 0.0625 in |
UL File #E56070 |