| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 30% Glass Filled |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Accutech Polycarbonate POL050G30L Glass Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.41 g/cc | 0.0509 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | MD; ASTM D955 |
| Melt Flow | 13 g/10 min | 13 g/10 min | ASTM D1238 |
| Ash | 30 % | 30 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Tensile Strength at Break | 124.0 MPa | 17980 psi | ASTM D638 |
| Tensile Strength, Yield | 125.0 MPa | 18130 psi | ASTM D638 |
| Elongation at Break | 6.0 % | 6.0 % | ASTM D638 |
| Elongation at Yield | 4.0 % | 4.0 % | ASTM D638 |
| Tensile Modulus | 4.899 GPa | 710.6 ksi | ASTM D638 |
| Flexural Strength | 195.9 MPa | 28420 psi | ASTM D790 |
| Flexural Modulus | 8.7984 GPa | 1276.1 ksi | ASTM D790 |
| Izod Impact, Notched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 145 °C | 293 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 140 °C | 284 °F |