| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Accutech Polypropylene Copolymer CP0436G5M25CL Glass/Mineral Reinforced Coupled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | MD; ASTM D955 |
| Melt Flow | 7.0 g/10 min | 7.0 g/10 min | ASTM D1238 |
| Ash | 30 % | 30 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 40 | 40 | ASTM D785 |
| Tensile Strength at Break | 22.0 MPa | 3190 psi | ASTM D638 |
| Tensile Strength, Yield | 25.0 MPa | 3630 psi | ASTM D638 |
| Elongation at Break | 8.0 % | 8.0 % | ASTM D638 |
| Elongation at Yield | 3.0 % | 3.0 % | ASTM D638 |
| Tensile Modulus | 2.699 GPa | 391.5 ksi | ASTM D638 |
| Flexural Strength | 38.0 MPa | 5510 psi | ASTM D790 |
| Flexural Modulus | 3.20 GPa | 464 ksi | ASTM D790 |
| Izod Impact, Notched | 0.854 J/cm | 1.60 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 140 °C | 284 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 86.1 °C | 187 °F |