| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Calcium Carbonate (CaCO3) Filler |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Accutech Polypropylene Copolymer CP0437C30L Calcium Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | MD; ASTM D955 |
| Melt Flow | 20 g/10 min | 20 g/10 min | ASTM D1238 |
| Ash | 30 % | 30 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 48 | 48 | ASTM D785 |
| Tensile Strength at Break | 11.0 MPa | 1600 psi | ASTM D638 |
| Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
| Elongation at Break | 60 % | 60 % | ASTM D638 |
| Elongation at Yield | 3.0 % | 3.0 % | ASTM D638 |
| Tensile Modulus | 1.300 GPa | 188.5 ksi | ASTM D638 |
| Flexural Strength | 19.0 MPa | 2760 psi | ASTM D790 |
| Flexural Modulus | 1.100 GPa | 159.5 ksi | ASTM D790 |
| Izod Impact, Notched | 3.42 J/cm | 6.40 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 77.8 °C | 172 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 52.2 °C | 126 °F |