| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.02 g/cc | 0.0368 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | MD; ASTM D955 |
| Melt Flow | 20 g/10 min | 20 g/10 min | ASTM D1238 |
| Ash | 20 % | 20 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 78 | 78 | ASTM D785 |
| Tensile Strength at Break | 27.0 MPa | 3920 psi | ASTM D638 |
| Tensile Strength, Yield | 33.0 MPa | 4790 psi | ASTM D638 |
| Elongation at Break | 16 % | 16 % | ASTM D638 |
| Elongation at Yield | 5.0 % | 5.0 % | ASTM D638 |
| Tensile Modulus | 2.499 GPa | 362.5 ksi | ASTM D638 |
| Flexural Strength | 42.0 MPa | 6090 psi | ASTM D790 |
| Flexural Modulus | 1.80 GPa | 261 ksi | ASTM D790 |
| Izod Impact, Notched | 0.352 J/cm | 0.660 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 116 °C | 241 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F |