| Category | Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded, Glass Reinforced |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Aclo Accutech SAN SAN930G40L Glass Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | MD; ASTM D955 |
| Melt Flow | 2.0 g/10 min | 2.0 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 118 | 118 | ASTM D785 |
| Tensile Strength at Break | 95.01 MPa | 13780 psi | ASTM D638 |
| Tensile Strength, Yield | 95.01 MPa | 13780 psi | ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | ASTM D638 |
| Elongation at Yield | 2.0 % | 2.0 % | ASTM D638 |
| Tensile Modulus | 6.8989 GPa | 1000.6 ksi | ASTM D638 |
| Flexural Strength | 133.0 MPa | 19290 psi | ASTM D790 |
| Flexural Modulus | 12.498 GPa | 1812.7 ksi | ASTM D790 |
| Izod Impact, Notched | 0.459 J/cm | 0.860 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 97.8 °C | 208 °F |