| Category | Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Cobalt Alloy , Nickel Alloy |
| Manufacturer | Alliance LLC |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Alliance A-5S Alnico Magnetic Material.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 6.90 - 7.30 g/cc | 0.249 - 0.264 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Vickers | 300 - 500 | 300 - 500 | |
| Tensile Strength, Ultimate | 80.0 - 300 MPa | 11600 - 43500 psi | |
| Modulus of Elasticity | 100 - 200 GPa | 14500 - 29000 ksi | |
| Compressive Strength | 300 - 400 MPa | 43500 - 58000 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 10.0 - 13.0 µm/m-°C @Temperature 20.0 °C |
5.56 - 7.22 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
| Specific Heat Capacity | 0.350 - 0.500 J/g-°C | 0.0837 - 0.120 BTU/lb-°F | |
| Thermal Conductivity | 10.0 - 200 W/m-K | 69.4 - 1390 BTU-in/hr-ft²-°F | |
| Maximum Service Temperature, Air | 450 °C | 842 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0000400 - 0.0000700 ohm-cm | 0.0000400 - 0.0000700 ohm-cm | |
| Magnetic Coercive Force, Hc | 590 Oe | 590 Oe | |
| 600 Oe | 600 Oe | Intrinsic | |
| Magnetic Remanence, Br | 10500 Gauss | 10500 Gauss | |
| Magnetic Maximum Energy Product, BH | 3.9 MGOe | 3.9 MGOe | |
| Curie Temperature | 850 °C | 1560 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Reversible Temp Coef., Bd | -0.016 %/°C | |
| Temperature Coefficient, Br | -0.025 %/°C | (20-100°C) |
| Temperature Coefficient, Hci | +0.01 %/°C | (20-100°C) |