| Category | Ceramic , Metal , Electronic/Magnetic Alloy |
| Manufacturer | Alliance LLC |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Alliance BCN-12 Bonded (Composite) Magnetic Material.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 5.60 - 6.00 g/cc | 0.202 - 0.217 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | |
| Modulus of Elasticity | 0.700 - 1.00 GPa | 102 - 145 ksi | |
| Compressive Strength | 80.0 - 120 MPa | 11600 - 17400 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 10.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
5.56 - 16.7 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
| Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | |
| Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
| Maximum Service Temperature, Air | 120 °C | 248 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.00100 - 0.00300 ohm-cm | 0.00100 - 0.00300 ohm-cm | |
| Magnetic Coercive Force, Hc | 5300 Oe | 5300 Oe | |
| 15000 Oe | 15000 Oe | Intrinsic | |
| Magnetic Remanence, Br | 6150 Gauss | 6150 Gauss | |
| Magnetic Maximum Energy Product, BH | 8.5 MGOe | 8.5 MGOe | |
| Curie Temperature | 300 - 470 °C | 572 - 878 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Reversible Temp Coef., Bd | -0.13 %/°C | |
| Reversible Temp Coef., Hd | -0.41 %/°C | |
| Temperature Coefficient, Br | -0.11 %/°C | (20-100°C) |
| Temperature Coefficient, Hci | -0.39 %/°C | (20-100°C) |