Ametek High Purity Nickel Strip 899L 1/4 Hard

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Ametek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ametek High Purity Nickel Strip 899L 1/4 Hard.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in pure nickel strip.Homogeneity, microcleanliness, and close composition control enhances weldability.Significantly low levels of surface oxides reduces die wear and provides excellent solderability.Excellent formability.Typical applications for rechargeable batteries: computers, cellular phones, power tools, electric vehicles, pagers, and camcorders.
Physical Properties Metric English Comments
Density 8.90 g/cc
0.322 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 70 - 80
70 - 80
Hardness, Vickers 120 - 151
120 - 151
Tensile Strength, Ultimate 379 - 483 MPa
55000 - 70100 psi
Tensile Strength, Yield 172 - 379 MPa

@Strain 0.200 %
24900 - 55000 psi

@Strain 0.200 %
Elongation at Break 20 - 35 %
20 - 35 %
typical
Poissons Ratio 0.31
0.31
Thermal Properties Metric English Comments
Thermal Conductivity 86.0 W/m-K

@Temperature 70.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 158 °F
Melting Point 1453 °C
2647 °F
Component Elements Properties Metric English Comments
Carbon, C 0.0050 - 0.020 %
0.0050 - 0.020 %
Copper, Cu <= 0.0050 %
<= 0.0050 %
Iron, Fe <= 0.050 %
<= 0.050 %
Manganese, Mn <= 0.070 %
<= 0.070 %
Nickel, Ni 99.8 %
99.8 %
Silicon, Si <= 0.0010 %
<= 0.0010 %
Sulfur, S <= 0.0010 %
<= 0.0010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000763 ohm-cm

@Temperature 20.0 °C
0.00000763 ohm-cm

@Temperature 68.0 °F
Curie Temperature 353 °C
667 °F