Arkema Group Evatane® 1005 VN 5 Ethylene Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer Arkema
Trade Name Evatane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Evatane® 1005 VN 5 Ethylene Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
EVA copolymer made by high pressure tubular process. Applications Grade for films with high transparency and high mechanical properties. Examples: coextrusion, stretch film, paper-stationary, fancy leather, geomembrane.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
Melt Flow 0.96 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.96 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.00 MPa
580 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Tensile Modulus 0.0500 GPa
7.25 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 90.0 °C
194 °F
10°C/min
Vicat Softening Point 66.0 °C
151 °F
50°C/hr; 50N
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.