Arkema Group Pebax® MV 1074 Polyether Block Amide (PEBA)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Pebax® MV 1074 Polyether Block Amide (PEBA).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Typical application: Breathable filmInformation provided by Arkema Group
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
Flexural Modulus 0.0900 GPa
13.1 ksi
Thermal Properties Metric English Comments
Melting Point 158 °C
316 °F