Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 266 PPO, 30% Glass Reinforced

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, 30% Glass Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 266 PPO, 30% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A general purpose, 30% glass reinforced PPO resin for injection molding applications.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 101 MPa
14600 psi
ATSM D638
Elongation at Break 4.1 %
4.1 %
ASTM D638
Flexural Modulus 7.20 GPa
1040 ksi
ASTM D790
Izod Impact, Notched 0.920 J/cm
1.72 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 148 °C
298 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 134 °C
273 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved