Ashley Polymers Ashlene® 528L-5G Nylon 66, 5% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 528L-5G Nylon 66, 5% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purpose glass fiber reinforced nylon, designed for parts requiring improved dimensional stability and higher strength than conventional resins.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 90.0 MPa
13100 psi
ATSM D638
Elongation at Break 7.5 %
7.5 %
ASTM D638
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
500 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
ASTM D648