Ashley Polymers Ashlene® 528MS/528SMS Nylon 66, MoS2 Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, MoS2 Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 528MS/528SMS Nylon 66, MoS2 Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A general purpose Molybdenum-disulfide filled nylon resin.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Water Absorption 1.0 %
1.0 %
24 hrs; ASTM D570
Water Absorption at Saturation 8.0 %
8.0 %
ASTM D570
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Ultimate 90.0 MPa
13100 psi
ATSM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 249 °C
480 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C
210 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved