| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled |
| Manufacturer | Asia Int'l Enterprise (Hong Kong) Limited |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Asia International Enterprise (Hong Kong) 60G6 Nylon 66, 30% Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.37 g/cc @Temperature 23.0 °C |
1.37 g/cc @Temperature 73.4 °F |
ASTM D792 |
| Filler Content | 30 % | 30 % | |
| Linear Mold Shrinkage | 0.0040 - 0.0090 cm/cm | 0.0040 - 0.0090 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 122 | 122 | ASTM D785 |
| Tensile Strength, Ultimate | 186 MPa | 27000 psi | 5mm/min; ASTM D638 |
| Elongation at Break | 2.0 % | 2.0 % | 5mm/min; ASTM D638 |
| Flexural Strength | 275 MPa | 39900 psi | 2.8mm/min; ASTM D790 |
| Flexural Modulus | 8.83 GPa | 1280 ksi | 2.8mm/min; ASTM D790 |
| Izod Impact, Notched | 1.08 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.02 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 261 °C | 502 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 260 °C | 500 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 250 °C | 482 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 250 - 300 °C | 482 - 572 °F | Cylinder Temperature |
| Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
| Dry Time | 4 - 6 hour | 4 - 6 hour |