Material Notes:
Non-lead stabilized general purpose jacketing compound with good low temperature properties. Recommended for a maximum service temperature of 80°C at a 15 mil wall thickness.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.34 g/cc
1.30 - 1.34 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 67 - 73
67 - 73
delayed; ASTM D-2240
Tensile Strength, Yield 12.4 MPa
1800 psi
ASTM D-638
Elongation at Yield 360 %
360 %
ASTM D-638
100% Modulus 0.00500 GPa
0.725 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -32.0 °C
-25.6 °F
ASTM D-746
Oxygen Index 23 %
23 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 168 °C
335 °F