Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 10870 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 10870 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purpose jacket compound recommended for 60C applications and also suited for 75C at a wall thickness of 30 mils and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.40 - 1.44 g/cc
1.40 - 1.44 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 84 - 90
84 - 90
delayed; ASTM D-2240
Tensile Strength, Yield 16.38 MPa
2375 psi
ASTM D-638
Elongation at Yield 263.8 %
263.8 %
Air Aging: 240 hours @ 100°C; 30 mil slabs; UL 1581
340 %
340 %
ASTM D-638
100% Modulus 0.00965 GPa
1.40 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -28.0 °C
-18.4 °F
ASTM D-746
Oxygen Index 23.5 %
23.5 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F
Users viewing this material also viewed the following: