| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
Polymer Resources TP-IM-G15 Polybutylene Terephthalate, 15% Glass Reinforced, Impact Modified
Polybutylene Terephthalate, 15% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
PolyOne Geon™ 170 Series 4195 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an..
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
PolyOne Geon™ 170 Series Adept E 49 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Adept E49 is a low molecular weight homopolymer dispersion resins intended for use in variety of plastisol applications and processes. It reduces scrap rates and manufacturing costs by extend..
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
PolyOne Geon™ 170 Series L120UF Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Ultrafine 170-L120UF is a high molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for thin..
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
PolyOne Geon™ Specialty Suspension Atlas S140 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Atlas S140 is high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical performance of end application for intsan..
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Dry Blend E6950 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
S&E Specialty Polymers TufTech™ GA-7565FR PVC Compound
Application: A 75°C Matte finish jacketing compound.Information provided by S&E Specialty Polymers
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
S&E Specialty Polymers TufTech™ GA-8705-03 Natural PVC Compound
Application: A 75°C, RoHS compliant, PVC based compound, suitable for Riser jacketing applications.Information provided by S&E Specialty Polymers
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D297 |
|
Parker Chomerics ParPHorm® 1800 Non-Conductive Form-in-Place Gasket
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
PolyOne Geon™ 120 Series 120X400 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® 120X400 is medium molecular weight resin providing a good balance of fusion temperatures and film physical properties. It gives good chemical foamability for producing medium to high density ..
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ISO 1183 |
|
Lehmann & Voss LUVOCOM® 1105-8002 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ISO 1183 |
|
Gromax BFM30-EL04B2 Nylon 6 30% Mineral Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
Samsung Cheil Industries Infino® AR-9301 PA, Glass Filled General Purpose
Information provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
Samsung Cheil Industries Infino® LS-3302 PC, 30% Glass Filled High Impact
High-impact resistant PC/GF with 30% GF reinforcement for camera body tubeInformation provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL EXNL1285 PPE+PS (Europe-Africa-Middle East)
Noryl* EXNL1285 Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
Teknor Apex Sinvicomp SRP 4606 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Medium Impact Resistance Uses: Conduit; Piping; Profiles Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Woodland Green 30233U/4 Concentrate Based In LLDPE
DescriptionPOLYBATCH® 30233U/4 is a green color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stability..
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
Cheng Yu Plastic T889G2 PBT, 20% Glass Fiber |
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | at 25°C |
|
Daikin NEOFLON ND-4 FEP Dispersion, Milky White
NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can ..
|
|||
| Specific Gravity | 1.40 - 1.44 g/cc | 1.40 - 1.44 g/cc | ASTM D792 |
|
Compuestos Dominicanos Polycom PW-103099 PVC Compound
Compuestos Dominicanos' rigid PVC compounds for the extrusion of pipes have excellent processing characteristics and are available in the form of pellets and dry-blend. Also available are compounds..
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
Colorite Polymers 8804 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
|
|||
| Specific Gravity | 1.40 - 1.44 g/cc | 1.40 - 1.44 g/cc | ASTM D-792 |
|
Axiall 8830 Moldings & Extrusions Flexible PVC
General purpose extrusion compound designed for use in weatherstrips, shapes, screen spline and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Atomite Whiting Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
Gharda Chemicals GATONE™ 5330CF Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Woodland Green 30233U/4 Concentrate Based In LLDPE
DescriptionPOLYBATCH® 30233U/4 is a green color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stability..
|
|||