Axiall 12792 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 12792 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purpose, 75°C rated non-lead stabilized jacket compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 76 - 82
76 - 82
delayed; ASTM D-2240
Tensile Strength, Yield 13.8 MPa
2000 psi
ASTM D-638
Elongation at Yield 292.7 %
292.7 %
Air Aging: 240 hours @ 100°C; 30 mil slabs; UL 1581
360 %
360 %
ASTM D-638
100% Modulus 0.00621 GPa
0.900 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D-746
Oxygen Index 23 %
23 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 171 °C
340 °F