Material Notes:
Georgia Gulf 9175 Amber 12 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It is a pre-colored amber compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.6 MPa
7200 psi
ASTM D-638
Tensile Modulus 2.90 GPa
420 ksi
ASTM D-638
Flexural Strength 89.6 MPa
13000 psi
ASTM D-790
Izod Impact, Notched 0.160 J/cm

@Thickness 6.35 mm
0.300 ft-lb/in

@Thickness 0.250 in
ASTM D-256
0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 115 kJ/m²
55.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 56.00 °C
132.8 °F
ASTM D-648
Descriptive Properties Value Comments
Equilibrium Torque, meter-grams 900
Brabender Plastograph, No. 6 Roller Head, 190°C Bath, 57-g. Charge; 60/43 rpm